| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.721 g/cc | 0.0260 lb/in³ | ASTM D1056 |
| Water Absorption | 3.0 % | 3.0 % | ASTM D570 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 0.689 MPa | 100 psi | ASTM D412 |
| Elongation at Break | 160 % | 160 % | ASTM D412 |
| Compressive Strength | 0.138 MPa | 20.0 psi | 0.25; ASTM D3675 |
| Compression Set | 2.0 % | 2.0 % | at 50%, 22 hrs @ 70°C; ASTM D1056 |
| <= 10 % @Temperature 100 °C |
<= 10 % @Temperature 212 °F |
at 50%, 22 hrs; ASTM D1056 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Flammability, UL94 | V-1 | V-1 | Rating dependent on color and thickness |
| V-0 | V-0 | Rating dependent on color and thickness | |
| Flammability Test | <= 25 | <= 25 | ASTM E162/D 3675 |
| Smoke Density | 1.5 min | 1.5 min | <20; ASTM E662 |
| 4.0 min | 4.0 min | <50; ASTM E662 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Thermal Resistance, ft2-h/BTU | 2.5 | ASTM C518 |
| Toxic Gas Emission | Pass | Bombardier SMP 800C |
| Vertical Flammability | Pass | FAR25.83(a)(1)(i) 12sec |
| Pass | FAR25.83(a)(1)(i) 60sec |