Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0960 g/cc | 0.00347 lb/in³ | |
Pyrotek SL-6 Fiberseal Blanket A more consistently thick, rigid, dense and insulating version of M-6.Dimensions610 mm x 15.2 m x 6 mm1219 mm x 15.2 m x 6 mm610 mm x 30.4 m x 12 mm1219 mm x 30.4 m x 12 mmApplicationsDie-cutting, f.. |
|||
Density | 0.0960 g/cc | 0.00347 lb/in³ | |
Pyrotek T-1 Fiber Seal Pre-cut Gasket A dark brown, very strong and tough material.Information provided by Pyrotek. |
|||
Density | 0.0960 - 0.128 g/cc | 0.00347 - 0.00462 lb/in³ | |
Pyrotek T-67B Fiberseal Blanket Soluble amorphous wool. Does not contain refractory ceramic fiber.Dimensions610 mm x 7.6 m1219 mm x 7.6 m6, 13, 51 mm thickApplicationsTrough repair Pot bake blanket Flexible joint packaging Carbon.. |
|||
Density | 0.0960 g/cc | 0.00347 lb/in³ | |
Pyrotek L-6 Fiberseal Blanket Lightweight, yet strong and durable needled blankets.Dimensions610 mm x 7.6 m1219 mm x 7.6 m6 - 51 mm thickApplicationsFurnace linings Gaskets Expansion joints Fire blanket Fire pillowsInformation p.. |
|||
Density | 0.0961 - 0.192 g/cc | 0.00347 - 0.00694 lb/in³ | |
Mid-Mountain Materials PADMAT® MT1000 Needled Fiberglass Mat Description: PADMAT® MT1000 fiberglass mat is comprised of high purity, high strength E-Glass fibers. These long fibers are mechanically needled into high strength, binderless insulation material.. |
|||
Density | 0.0961 g/cc | 0.00347 lb/in³ | Layered |
Unifrax Anchor-Loc® 3000 Ceramic Fiber Modules The Anchor-Loc® module system is a family of ceramic fiber module products designed to meet a wide range of application requirements in a variety of heat processing vessels.Ceramic fiber modules us.. |
|||
Density | 0.0961 g/cc | 0.00347 lb/in³ | Available |
Unifrax Fiberfrax® Durablanket® HP-S Ceramic Fiber Insulator Fiberfrax Durablanket HP-S insulation is a needled blanket made from spun Fiberfrax ceramic fibers. Durablanket HP-S insulation combines all of the physical characteristics offered by Durablanket S.. |
|||
Density | 0.0961 g/cc | 0.00347 lb/in³ | |
Unifrax Fibermax® Needled Blanket Fibermax® Needled Blankets are high temperature, light weight and flexible products manufactured from polycrystalline mullite fiber that can be exposed to temperatures up to 1600°C (2912°F). Fib.. |
|||
Density | 0.0961 g/cc | 0.00347 lb/in³ | Nominal |
Unifrax FyreWrap® Elite™ 1.5 Duct Insulation Grease Duct ASTM E2336 System Unifrax's FyreWrap ™ 1.5 Duct Insulation is a two-layer flexible enclosure for one- and two-hour rated commercial kitchen grease ducts and hazardous exhaust ducts including chemical fume ducts. Fy.. |
|||
Density | 0.0961 g/cc | 0.00347 lb/in³ | Nominal |
Unifrax FyreWrap® Elite™ 1.5 Duct Insulation Grease Duct Single-Layer System Insulation Unifrax's FyreWrap ™ 1.5 Duct Insulation is a single-layer flexible enclosure for 1- and 2-hour fire-rated commercial kitchen grease ducts and hazardous exhaust ducts including chemical fume ducts... |
|||
Density | 0.0961 g/cc | 0.00347 lb/in³ | Nominal |
Hexcel® HexWeb® CR III 1/4-5052-.003 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Density | 0.0961 g/cc | 0.00347 lb/in³ | |
Hexcel® HexWeb® HRH-10 - 3/16 - 6.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Density | 0.0961 g/cc | 0.00347 lb/in³ | |
Hexcel® HexWeb® HRH-327 - 3/16 - 6.0 Fiberglass Reinforced Polyimide Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a.. |
|||
Density | 0.0961 g/cc | 0.00347 lb/in³ | |
Hexcel® HexWeb® HRH-36 - 1/8 - 6.0 Para-Aramid/Phenolic Core Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.Features: Mechanical properties equivalent to KOREX®; Low.. |
|||
Density | 0.0961 g/cc | 0.00347 lb/in³ | |
Hexcel® HexWeb® HRP - 3/8 - 6.0 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Density | 0.0961 g/cc | 0.00347 lb/in³ | Available |
Unifrax Fiberfrax® Durablanket® S Ceramic Fiber Insulator Fiberfrax Durablanket S insulation is a strong, lightweight, flexible needled blanket that is made from spun ceramic fibers. Available in a wide variety of thicknesses, widths and densities, Durabl.. |
|||
Density | 0.0960 g/cc | 0.00347 lb/in³ | Molded density, ASTM D3574-A |
Covestro Bayfill® 310 Polyurethane Semi-Rigid Foam, MDI-based 2-Component Liquid System Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Density | 0.0960 g/cc | 0.00347 lb/in³ | Molded density, ASTM D3574-A |
Covestro Bayfill® 312 Polyurethane Semi-Rigid Foam, MDI-based 2-Component Liquid System Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Density | 0.0960 g/cc | 0.00347 lb/in³ | |
3M 4462B Double Coated Polyethylene Foam Tape 3M™ Double Coated Polyethylene Foam Tapes 4462W, 4462B, 4466W and 4466B combine a conformable closed cell foam with a rubber adhesive that provides high initial adhesion to a variety of surfaces in.. |
|||
Density | 0.0960 g/cc | 0.00347 lb/in³ | |
3M 4462W Double Coated Polyethylene Foam Tape 3M™ Double Coated Polyethylene Foam Tapes 4462W, 4462B, 4466W and 4466B combine a conformable closed cell foam with a rubber adhesive that provides high initial adhesion to a variety of surfaces in.. |
|||
Density | 0.0960 g/cc | 0.00347 lb/in³ | |
Pyrotek M-3 Fiber Seal Pre-cut Gasket A resin-coated felt. Repels water.Information provided by Pyrotek. |
|||
Density | 0.0961 g/cc | 0.00347 lb/in³ | Nominal |
Hexcel® HexWeb® CR-PAA™ 1/4-5052-0.003 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |