Pyrotek L-6 Fiberseal Blanket

Category Ceramic
Manufacturer Pyrotek, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek L-6 Fiberseal Blanket.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Lightweight, yet strong and durable needled blankets.Dimensions610 mm x 7.6 m1219 mm x 7.6 m6 - 51 mm thickApplicationsFurnace linings Gaskets Expansion joints Fire blanket Fire pillowsInformation provided by Pyrotek.
Physical Properties Metric English Comments
Density 0.0960 g/cc
0.00347 lb/in³
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1427 °C
2601 °F