Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.875 - 2.24 g/cc | 0.0316 - 0.0809 lb/in³ | Average value: 1.11 g/cc Grade Count:307 |
Overview of materials for Cyanoacrylate Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Density | 0.970 - 2.24 g/cc | 0.0350 - 0.0809 lb/in³ | Average value: 1.32 g/cc Grade Count:46 |
Overview of materials for Silicone, RTV, Encapsulation Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Encapsulation Grade". Each property range of values reported is minimum and maximum value.. |
|||
Density | 2.18 - 2.24 g/cc | 0.0788 - 0.0809 lb/in³ | molded; ASTM D792 |
Guarniflon PTFE G436 Polytetrafluoroethylene 3% Molybdenum Disulfide PTFE G Standard Compound with molybdenum disulphite. Enhanced non-stick properties. Low static coefficient of friction. Fairly good resistance to deformation. Applications: Guide bands. Details ne.. |
|||
Density | 2.22 - 2.24 g/cc | 0.0802 - 0.0809 lb/in³ | extruded; ASTM D792 |
Guarniflon PTFE G405 Polytetrafluoroethylene 25% Glass Fiber PTFE G Standard Compound with glass fiberProperties: Enhanced wear resistance. Enhanced chemical resistance (except for alkali and hydrofluoric acid).Applications: Valve seats, seals, bearings, re.. |