Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.00545 - 1.88 g/cc | 0.000197 - 0.0679 lb/in³ | Average value: 1.35 g/cc Grade Count:132 |
Overview of materials for Polyimide This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Density | 1.69 - 1.88 g/cc | 0.0611 - 0.0679 lb/in³ | Average value: 1.78 g/cc Grade Count:105 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
Density | 1.73 - 1.88 g/cc | 0.0626 - 0.0678 lb/in³ | |
Saint-Gobain Chemfab® 1584N PTFE Coated Fiberglass Conveyor Belting Description: General Notes on Saint Gobain Belting Products:Saint Gobain Performance Plastics developed its belting materials for applications that require superior release characteristics, permeabi.. |
|||
Density | 1.76 - 1.88 g/cc | 0.0636 - 0.0679 lb/in³ | ASTM D792 |
Zeus PVDF Tubing PVDF, polyvinylidene fluoride, delivers high performance at a competitive cost. Its inherent purity positions it as ideal for a variety of applications which involve extreme conditions. PVDF is char.. |
|||
Density | 1.47 - 1.88 g/cc | 0.0531 - 0.0679 lb/in³ | Average value: 1.57 g/cc Grade Count:45 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Density | 1.44 - 1.88 g/cc | 0.0520 - 0.0679 lb/in³ | Average value: 1.71 g/cc Grade Count:25 |
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% .. |
|||
Density | 1.68 - 1.88 g/cc | 0.0607 - 0.0679 lb/in³ | Molded |
Bulk Molding Compounds BMC T40(20) Die Casting Replacement Grade Molding Compound BMC T40(20) was formulated as a direct replacement for aluminum die casting applications. T40(20) is UL recognized. Excellent mechanical properties and dimensional control allow molded parts to ma.. |