Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.70 - 1.73 g/cc | 0.0614 - 0.0625 lb/in³ | Liquid |
Oceanchem Group Calcium Bromide (CaBr2) Molecular Formula: CaBr2Cas No.: 7789-41-5Use: Calcium Bromide and its formuulated brines are mainly used as completion, workover and packer fluids in oil drilling field.Properties: This product is .. |
|||
Density | 1.13 - 1.73 g/cc | 0.0408 - 0.0625 lb/in³ | Average value: 1.30 g/cc Grade Count:55 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Density | 1.20 - 1.73 g/cc | 0.0434 - 0.0625 lb/in³ | Average value: 1.51 g/cc Grade Count:35 |
Overview of materials for Acetal Copolymer, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values .. |
|||
Density | 1.16 - 1.73 g/cc | 0.0419 - 0.0625 lb/in³ | Average value: 1.38 g/cc Grade Count:70 |
Overview of materials for Polycarbonate, Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val.. |
|||
Density | 1.18 - 1.73 g/cc | 0.0426 - 0.0625 lb/in³ | Average value: 1.33 g/cc Grade Count:5 |
Overview of materials for Nylon 66/6, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl.. |
|||
Density | 1.23 - 1.73 g/cc | 0.0444 - 0.0625 lb/in³ | Average value: 1.45 g/cc Grade Count:117 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Density | 1.25 - 1.73 g/cc | 0.0452 - 0.0625 lb/in³ | Average value: 1.53 g/cc Grade Count:50 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |