Oceanchem Group Calcium Bromide (CaBr2)

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Oceanchem Group
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oceanchem Group Calcium Bromide (CaBr2).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Molecular Formula: CaBr2Cas No.: 7789-41-5Use: Calcium Bromide and its formuulated brines are mainly used as completion, workover and packer fluids in oil drilling field.Properties: This product is white grain or cake crystal; it is free of smell and tastes salty and slightly bitter. It can dissolve in water and ethand or actone, hardly dissolves in aether or chloroform. It will turn yellow if placed in the air for a long time. It is very quick hygroscopic, its aqueous solution is neutral.Storage and Handling: Product containers from damage and keep them well closed. Store in a cool, well-ventilated, dry and shaded storehouse. Avoid inhalation, ingestion and contact with the eyes and skin.Information Provided by Oceanchem Group
Physical Properties Metric English Comments
Density 1.70 - 1.73 g/cc
0.0614 - 0.0625 lb/in³
Liquid
pH 6.0 - 8.0
6.0 - 8.0
Solid
7.0 - 9.0
7.0 - 9.0
Liquid
Molecular Weight 199.88 g/mol
199.88 g/mol
Thermal Properties Metric English Comments
Melting Point 730 °C
1350 °F
Boiling Point 806 - 812 °C
1480 - 1490 °F
Processing Properties Metric English Comments
Moisture Content <= 3.0 %
<= 3.0 %
Solid
Descriptive Properties Value Comments
Appearance Clear colorless to pack yellow
Liquid
White grain or lumpy
Solid
Assay (%) 52
Liquid; as CaBr<sub>2</sub>
95
Solid; as CaBr<sub>2</sub>
CAS Number 7789-41-5
Chloride (%) <0.3
Liquid
<0.5
Solid
Molecular Formula CaBr2
Sulphate (%) <0.03
Liquid
<0.05
Solid
Water-insoluble (%) <0.5
Solid