Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.890 - 1.21 g/cc | 0.0322 - 0.0437 lb/in³ | Average value: 1.06 g/cc Grade Count:130 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Density | 0.923 - 1.21 g/cc | 0.0333 - 0.0437 lb/in³ | Average value: 0.944 g/cc Grade Count:94 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum .. |
|||
Density | 1.16 - 1.21 g/cc | 0.0420 - 0.0437 lb/in³ | |
Lord Adhesives 17 Mix-In Accelerator for 200, 400, 500 Series Lord Adhesives 17 Mix-In Accelerator for 200, 400, 500 SeriesLord Accelerator 17 mix-in accelerator for Lord 200, 400 and 500 series acrylic adhesives. Use at a 10:1 ratio. |
|||
Density | 1.15 - 1.21 g/cc | 0.0415 - 0.0437 lb/in³ | |
Dow BETAMATE™ 1496 V Epoxy BETAMATE™ 1496 V is a one component, epoxy based adhesive especially developed for the body shop. The product has the following properties: Good rheology performance (Wash-out resistant, excelle.. |
|||
Density | 1.17 - 1.21 g/cc | 0.0423 - 0.0437 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 0145/R Flexible PVC, Injection Molding, Lead Free Technical items with rubber/PU |
|||
Density | 1.17 - 1.21 g/cc | 0.0423 - 0.0437 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 58 Flexible PVC, Injection Molding for Footwear Antislip soles |
|||
Density | 1.17 - 1.21 g/cc | 0.0423 - 0.0437 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 59/C Flexible PVC, Injection Molding for Footwear Sandals |
|||
Density | 1.17 - 1.21 g/cc | 0.0423 - 0.0437 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 60/B Flexible PVC, Injection Molding for Footwear Bicoloured soles |
|||
Density | 1.17 - 1.21 g/cc | 0.0423 - 0.0437 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 64/BT Flexible PVC, Injection Molding for Footwear Soles for cold climates |
|||
Density | 1.17 - 1.21 g/cc | 0.0423 - 0.0437 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 650 Flexible PVC, Injection Molding for Footwear Anti-slip soles |
|||
Density | 1.17 - 1.21 g/cc | 0.0423 - 0.0437 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 66/BT Flexible PVC, Injection Molding for Footwear Soles for cold climates |
|||
Density | 1.17 - 1.21 g/cc | 0.0423 - 0.0437 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 67/BT Flexible PVC, Injection Molding for Footwear Soles for cold climates |
|||
Density | 1.17 - 1.21 g/cc | 0.0423 - 0.0437 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 62 Medical Flexible PVC, Extrusion Tubolar apparatus and peristaltic pump segments |
|||
Density | 1.17 - 1.21 g/cc | 0.0423 - 0.0437 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 62/H Medical Flexible PVC, Extrusion Technical tubes and peristaltic pump segments no DOP |
|||
Density | 1.17 - 1.21 g/cc | 0.0423 - 0.0437 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 62/OP Medical Flexible PVC, Extrusion Tubolar apparatus and peristaltic pump segments |
|||
Density | 1.17 - 1.21 g/cc | 0.0423 - 0.0437 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 63 Medical Flexible PVC, Extrusion Tubolar apparatus |
|||
Density | 1.17 - 1.21 g/cc | 0.0423 - 0.0437 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 69/T Medical Flexible PVC, Extrusion Technical tubes no DOP |
|||
Density | 1.17 - 1.21 g/cc | 0.0423 - 0.0437 lb/in³ | ISO R 1183 |
Fainplast Compounds PG 60 Flexible PVC, Extrusion Modified with Rubber Gaskets modified with rubber |
|||
Density | 1.17 - 1.21 g/cc | 0.0423 - 0.0437 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 60 Flexible PVC, Transparent Extrusion Transparent profiles |
|||
Density | 1.17 - 1.21 g/cc | 0.0423 - 0.0437 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 66/A Flexible PVC, Transparent Extrusion Profiles, UL Class V2 |
|||
Density | 1.17 - 1.21 g/cc | 0.0423 - 0.0437 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 75/SN Flexible PVC, Transparent Extrusion Transparent and flexible sheets |
|||
Density | 1.17 - 1.21 g/cc | 0.0423 - 0.0437 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 5010 Flexible PVC, Lead Free Gaskets for frames |
|||
Density | 1.17 - 1.21 g/cc | 0.0423 - 0.0437 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 55/K Flexible PVC, Lead Free Inner tube |
|||
Density | 1.17 - 1.21 g/cc | 0.0423 - 0.0437 lb/in³ | ISO R 1184 |
Fainplast Compounds KLT 79 Flexible PVC, Insulation Transparent Cables Lead Free Transparent cables (90°C) |
|||
Density | 1.17 - 1.21 g/cc | 0.0423 - 0.0437 lb/in³ | Average value: 1.20 g/cc Grade Count:74 |
Overview of materials for Cellulose Acetate Propionate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Propionate, Molded". Each property range of values reported is minimum and maximum val.. |
|||
Density | 1.17 - 1.21 g/cc | 0.0423 - 0.0437 lb/in³ | ISO R 1183 |
Fainplast Compounds PG 62/K Flexible PVC, Extrusion Modified with Rubber Gaskets modified with rubber opaque surface |
|||
Density | 1.17 - 1.21 g/cc | 0.0423 - 0.0437 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 62 Flexible PVC, Transparent Extrusion Transparent profiles |
|||
Density | 1.17 - 1.21 g/cc | 0.0423 - 0.0437 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 785A PCL TPU Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech |
|||
Density | 1.05 - 1.21 g/cc | 0.0379 - 0.0437 lb/in³ | Average value: 1.13 g/cc Grade Count:5 |
Overview of materials for Polypropylene with Glass Fiber + PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + PTFE". Each property range of values reported is minimum and maximum va.. |
|||
Density | 0.951 - 1.21 g/cc | 0.0344 - 0.0437 lb/in³ | Average value: 1.03 g/cc Grade Count:22 |
Overview of materials for Polypropylene, Wood Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Wood Filled". Each property range of values reported is minimum and maximum values of app.. |