Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.11 - 1.12 g/cc | 0.0401 - 0.0405 lb/in³ | Average value: 1.12 g/cc Grade Count:5 |
Overview of materials for Nylon 6/69 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6/69". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Density | 1.12 - 1.12 g/cc @Temperature >=250 °C |
0.0405 - 0.0405 lb/in³ @Temperature >=482 °F |
Average value: 1.12 g/cc Grade Count:1 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |
|||
Density | 1.10 - 1.12 g/cc | 0.0397 - 0.0405 lb/in³ | ASTM D1505 |
Specialty Coating Systems Parylene N Poly (P-Xylylene) Coating Parylene N, poly(para-xylylene), is a completely linear, highly crystalline material. Parylene N is a primary dielectric, exhibiting a very low dissipation factor, high dielectric strength, and a lo.. |
|||
Density | 1.08 - 1.12 g/cc | 0.0390 - 0.0405 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 265A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Density | 1.08 - 1.12 g/cc | 0.0390 - 0.0405 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 365A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |
|||
Density | 1.08 - 1.12 g/cc | 0.0390 - 0.0405 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 465A Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Density | 1.08 - 1.12 g/cc | 0.0390 - 0.0405 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 582A Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |
|||
Density | 1.08 - 1.12 g/cc | 0.0390 - 0.0405 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 665A Polyester and Polyether based TPU Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Density | 1.09 - 1.12 g/cc | 0.0394 - 0.0405 lb/in³ | Average value: 1.11 g/cc Grade Count:11 |
Overview of materials for Ethyl Cellulose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Ethyl Cellulose, Molded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Density | 1.08 - 1.12 g/cc | 0.0390 - 0.0405 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 782A PCL TPU Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech |