Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.942 - 0.952 g/cc | 0.0340 - 0.0344 lb/in³ | ISO 1183 |
Polyplastic Torlen® PE 2K 901 High Density Polyethylene, Carbon Filled Information provided by PolyPlastic Group. |
|||
Density | 0.948 - 0.952 g/cc | 0.0342 - 0.0344 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4050Q (50403) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.948 - 0.952 g/cc | 0.0342 - 0.0344 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4850B (504H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.948 - 0.952 g/cc | 0.0342 - 0.0344 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4851B (504H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.948 - 0.952 g/cc | 0.0342 - 0.0344 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 6250D (506H4) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.948 - 0.952 g/cc | 0.0342 - 0.0344 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 6750H (506H8) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.948 - 0.952 g/cc | 0.0342 - 0.0344 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4550N (50401M) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.948 - 0.952 g/cc | 0.0342 - 0.0344 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4650N (50401N) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.949 - 0.952 g/cc | 0.0343 - 0.0344 lb/in³ | |
Kazanorgsintez 273-385 High Density Polyethylene Composite, Film Grade Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions are .. |
|||
Density | 0.948 - 0.952 g/cc | 0.0342 - 0.0344 lb/in³ | DIN 53479 |
Iran Petrochemical (PCC) Arak I2 HDPE Information provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.950 - 0.952 g/cc | 0.0343 - 0.0344 lb/in³ | ASTM D792-00 |
Ipiranga Petrochem GP 100 OR HDPE The resin GP 100 OR is a high density polyethylene compounding with high molar mass, specially developed for the manufacturing of extruded pipes for gas distribution. It is produced with bimodal tec.. |
|||
Density | 0.941 - 0.952 g/cc | 0.0340 - 0.0344 lb/in³ | Average value: 0.946 g/cc Grade Count:26 |
Overview of materials for High Density Polyethylene (HDPE), Rotational Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Rotational Molding Grade". Each property range of values reported is m.. |