Physical Properties Metric English Comments
Density 0.910 - 0.930 g/cc
0.0329 - 0.0336 lb/in³
ISO 1183
Polyplastic Armobond® PE 2K Polyethylene Adhesive Compound
Information provided by PolyPlastic Group.
Density 0.926 - 0.930 g/cc
0.0335 - 0.0336 lb/in³
Base Resin; ASTM D1505
NIZHNEKAMSKNEFTEKHIM PE 4028X (28435) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Density 0.900 - 0.930 g/cc
0.0325 - 0.0336 lb/in³
TPI Method
IRPC Polimaxx Polene PE100N Polypropylene Wax
APPLICATIONS: CARRIER FOR PIGMENT CONCENTRATES, LUBRICANT FOR PLASTICS, RUBBER EXTRUSION, HOT MELT ADHESIVE, PAPER COATING
Density 0.900 - 0.930 g/cc
0.0325 - 0.0336 lb/in³
TPI Method
IRPC Polimaxx Polene PE200N Polypropylene Wax
APPLICATIONS: CARRIER FOR PIGMENT CONCENTRATES, LUBRICANT FOR PLASTICS, RUBBER EXTRUSION, HOT MELT ADHESIVE, PAPER COATING
Density 0.900 - 0.930 g/cc
0.0325 - 0.0336 lb/in³
TPI Method
IRPC Polimaxx Polene PE220NSC Polypropylene Wax
APPLICATIONS: CARRIER FOR PIGMENT CONCENTRATES, LUBRICANT FOR PLASTICS, RUBBER EXTRUSION, HOT MELT ADHESIVE, PAPER COATING
Density 0.900 - 0.930 g/cc
0.0325 - 0.0336 lb/in³
TPI Method
IRPC Polimaxx Polene PE250N Polypropylene Wax
APPLICATIONS: CARRIER FOR PIGMENT CONCENTRATES, LUBRICANT FOR PLASTICS, RUBBER EXTRUSION, HOT MELT ADHESIVE, PAPER COATING
Density 0.900 - 0.930 g/cc
0.0325 - 0.0336 lb/in³
TPI Method
IRPC Polimaxx Polene PE300N Polypropylene Wax
APPLICATIONS: CARRIER FOR PIGMENT CONCENTRATES, LUBRICANT FOR PLASTICS, RUBBER EXTRUSION, HOT MELT ADHESIVE, PAPER COATING
Density 0.870 - 0.930 g/cc
0.0314 - 0.0336 lb/in³
ASTM D 792
Karina 55/200-TR Kariprene Cristal
Thermoplastic rubber compound, recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Density 0.870 - 0.930 g/cc
0.0314 - 0.0336 lb/in³
RP-1008
Solvay RHODOLINE® DF 540 Surfactant
Description: Highly effective white oil defoamer for latex processing.Identification: DEFOAMERAvailable in: North AmericaApplications: RHODOLINE© DF 540 is a general purpose silicone-free, high a..
Density 0.919 - 0.930 g/cc
0.0332 - 0.0336 lb/in³
Average value: 0.922 g/cc Grade Count:5
Overview of materials for Low Density Polyethylene (LDPE), Sheet/Profile extrusions
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Sheet/Profile extrusions". Each property range of values reported is mi..
Density 0.928 - 0.930 g/cc
0.0335 - 0.0336 lb/in³
ASTM D1505
Petroquimica Triunfo Trithene® SX 9003 MDPE - Blow Molding
The Trithene® SX 9003 resin is a medium density polyethylene (MDPE) with high molecular weight that presents excellent mechanical properties, thermal stability and high stiffness when compared with..