Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.917 - 0.919 g/cc | 0.0331 - 0.0332 lb/in³ | |
Kazanorgsintez 11503-070 UUP Low Density Polyethylene Production Method: LDPE is produced by high pressure ethylene polymerization in tubular reactors. Application: Designed for packaging and production of products designed for food contact, toy p.. |
|||
Density | 0.913 - 0.919 g/cc | 0.0330 - 0.0332 lb/in³ | ASTM D4883 |
Westlake Epolene® C-17 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer Product Description: Epolene C-17 is a branched low density polyethylene with a relatively high melt point and viscosity compared to other Epolene C-type Polymers. It is useful to modify paraffin wa.. |
|||
Density | 0.915 - 0.919 g/cc | 0.0331 - 0.0332 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® JX 7300 LDPE - Injection Molding The Trithene® JX 7300 resin is a low-density polyethylene (LDPE) with outstanding flow ability and flexibility. Those attributes are especially important to meet the requirements for fast injection.. |
|||
Density | 0.917 - 0.919 g/cc | 0.0331 - 0.0332 lb/in³ | |
Kazanorgsintez 11503-070 High Pressure Polyethylene Production Method: HDPE is produced by high pressure ethylene polymerization in tubular reactors. Application: Intended for production of bags, pipes, fittings, articles designed for food contac.. |