Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.80 g/cc | 0.318 lb/in³ | |
Materion Alloy 390 Beryllium Nickel Strip Alloy 390 was specifically designed for high power applications, providing a unique combination of high strength and high conductivity. Increasing power requirements are driving the need for lower c.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
Materion Brush 60™ 3/4 HT Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation afte.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
Special Metals MONEL® Alloy 400 A nickel-copper alloy with high strength and excellent corrosion resistance in a range of media including sea water, hydrofluoric acid, sulfuric acid, and alkalis. Used for marine engineering, chem.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
Goodfellow Nickel Base Magnetic Shielding Alloy - Mu Metal High Nickel magnetically soft alloy used for magnetic shielding, high quality but low noise audio frequency transformers, ground fault interrupter cores, anti-shoplifting devices, tape recorder head.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | Annealed |
Eagle Brass 220 Commercial Bronze, 1/2 Hard CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | Annealed |
Eagle Brass 220 Commercial Bronze, Extra Hard CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | Annealed |
Eagle Brass 220 Commercial Bronze, Extra Spring CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | Annealed |
Eagle Brass 220 Commercial Bronze, Spring CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | Annealed |
Eagle Brass 519 Phosphor Bronzes 6%, 1/4 Hard Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | Annealed |
Eagle Brass 519 Phosphor Bronzes 6%, Hard Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | Annealed |
Eagle Brass 521 Phosphor Bronzes 8% C, 1/4 Hard Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
CLAL-MSX ARCAP Anticorrosion AP1 0 Annealed, Drawn Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. Its machineability is one of the best of all of the corrosion resistant alloys. The very good machineability of.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
CLAL-MSX ARCAP Anticorrosion AP1 H12 1/2 hard, Rolled Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
CLAL-MSX ARCAP Anticorrosion AP1C H13 3/4 hard, Drawn Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
CLAL-MSX DECLAFOR® 1015 TB Wire quenched Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
CLAL-MSX DECLAFOR® 1015 TD2 Wire quenched/Cold Rolled Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
CLAL-MSX DECLAFOR® 1015 TD4 Wire quenched/Cold Rolled Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
CLAL-MSX DECLAFOR® 1015 TDX Rod quenched/Cold Rolled Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
CLAL-MSX DECLAFOR® 1015 TH1 Rod quenched/Cold Rolled/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
CLAL-MSX DECLAFOR® 1015 THX Rod quenched/Cold Rolled/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
CLAL-MSX ARCAP Anticorrosion AP1 H13 3/4 hard, Rolled Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
CLAL-MSX ARCAP Anticorrosion AP1C H11 1/4 hard, Drawn Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
CLAL-MSX ARCAP Anticorrosion AP1C H14 4/4 hard, Rolled Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
CLAL-MSX ARCAP Anticorrosion AP1C H15 Spring, Drawn Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
CLAL-MSX ARCAP Anticorrosion AP1D H14 4/4 hard, Drawn Copper Alloy, Wire and rod, 2.5< diameter< 5 High Corrosion Resistance: ARCAP alloys are very corrosion resistant to the majority of chemical and physical environments. CLAL can provide data for the corrosion resistance of ARCAP alloys. In par.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
CLAL-MSX ARCAP Anticorrosion AP1D H14 4/4 hard, Drawn Copper Alloy, Wire and rod, diameter High Corrosion Resistance: ARCAP alloys are very corrosion resistant to the majority of chemical and physical environments. CLAL can provide data for the corrosion resistance of ARCAP alloys. In par.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
CLAL-MSX DECLAFOR® 1015 TD1 Rod quenched/Cold Rolled Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
Cadi 1 MOLD-MOR™ A very hard heat treatable copper alloy with moderate electrical conductivity. C18000 offers excellent value for the properties it offers. C18000 is a viable substitute for C17500 and C17510 for m.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
Kennametal Stellite Stellite® 4 Cobalt Chromium Alloy The higher tungsten content of Stellite alloy 4 gives improved high temperature properties and an increase in abrasive wear resistance over Stellite alloy 6, but not as good as Stellite alloy 12 or .. |