Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.60 - 3.65 g/cc | 0.130 - 0.132 lb/in³ | Sintered Density |
Nabaltec GRANALOX® NM 9216 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Density | 3.60 g/cc | 0.130 lb/in³ | Sintered Density |
Nabaltec NABALOX® NO 115-71 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.60 g/cc | 0.130 lb/in³ | |
Nabaltec NABALOX® NO 201 Calcined Aluminum Oxide NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.60 g/cc | 0.130 lb/in³ | |
Nabaltec NABALOX® NO 201P Soft Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.60 g/cc | 0.130 lb/in³ | Sintered Density |
Nabaltec NABALOX® NO 315 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.60 g/cc | 0.130 lb/in³ | |
NanoScale NanoActive® Magnesium Oxide Plus NanoActive MgO is produced using proprietary processes to obtain very high specific surface area (over 600 m2/g), small crystallite size, high porosity material possessing high chemical reactivity a.. |
|||
Density | 3.60 g/cc | 0.130 lb/in³ | calculated from bulk density after subtracting pore volume |
MarkeTech Repton 115 Aluminum Oxide Brand 115 features: High Density and Purity.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even whe.. |
|||
Density | 3.60 g/cc | 0.130 lb/in³ | |
MarkeTech Spinel (MgAl2O4) Single Crystal Substrate Data provided by the supplier, MarkeTech International.Developed for deposition of III-V nitrides for LEDs, Lasers, etc. Standard orientation: ; GaN Lattice Mismatch 9%. |
|||
Density | 3.60 g/cc | 0.130 lb/in³ | |
Schott F2 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.60 g/cc | 0.130 lb/in³ | |
Schott F2HT Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 3.60 g/cc | 0.130 lb/in³ | |
CeramTec 771 94% Alumina (Al2O3) Te value is 840°C. Hasselman Thermal Shock value is 200 K.Data provided by CeramTec North America. |
|||
Density | 3.60 g/cc | 0.130 lb/in³ | |
American Elements Magnesium Oxide Nanopowder General DescriptionMagnesium Oxide Nanoparticles or Magnesia Nanoparticles (MgO) Nanoparticles, nanodots or nanopowder are spinel, high surface area particles. Nanoscale Magnesium Oxide Nanoparticle.. |
|||
Density | 3.60 g/cc | 0.130 lb/in³ | ASTM C20 |
CoorsTek AD-90 Alumina (nom. 90% Al2O3) Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Density | 3.60 g/cc | 0.130 lb/in³ | ASTM D1475 |
Aptek 2312-PMF Electrically conductive, low modulus adhesive Premixed-frozen, electrically conductive, low modulus adhesiveAPTEK 2312-PMF is a one component, premixed-frozen, silver filled, electrically conductive soft paste adhesive. It is designed to bond m.. |
|||
Density | >= 3.60 g/cc | >= 0.130 lb/in³ | |
Advanced Ceramics ALC 1081 (C-786) Alumina Information provided by Advanced Ceramics Limited (ACL) |
|||
Density | 3.60 g/cc | 0.130 lb/in³ | |
BASF Paliotan® Yellow L 2045 Color Additive Description: Pigment combination based on Bismuth VanadatSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Amine curing system and Airdrying systems.Information provided b.. |
|||
Density | 3.60 g/cc | 0.130 lb/in³ | |
Loctite® 3883 Stencil Print Isotropic Epoxy Adhesive Electrically Conductive BondersLoctite® Electrically Conductive Adhesives are used in a variety of applications where electrical connectivity is needed, providing a conductive path where traditiona.. |
|||
Density | 3.60 g/cc | 0.130 lb/in³ | |
Loctite® 3889 Rapid Cure Isotropic Epoxy Adhesive Electrically Conductive BondersLoctite® Electrically Conductive Adhesives are used in a variety of applications where electrical connectivity is needed, providing a conductive path where traditiona.. |