Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Mykroy/Mycalex MM 501 Molding Grade Glass-bonded Mica Composite Natural mica filler. Does not burn. ROHS Compliant.This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting demands of technical markets, worldwide.. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Mykroy/Mycalex MM 561 Molding Grade Glass-bonded Mica Composite Synthetic mica filler. Does not burn. Good radiation resistance (3 x 10^10 Rads-Cobalt). ROHS CompliantThis ceramoplastic material is a versatile and efficient insulating material designed to meet.. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Rogers Corporation RO3006 Ceramic-Filled PTFE Composite, High Frequency Circuit Material Features and Benefits: |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Potters Industries Spheriglass® EMB-10 Low Alkaline Boro-Silicate Solid Glass Microspheres Spheriglass® solid glass microspheres have been developed as a filler for paints, coatings, and films.Information provided by Potters Industries. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Pyrotek Pinnacle Thermocouple Protection Tubes O'-Sialon (Bonded Silicon Carbide) TCPT The robust properties of Pinnacle Thermocouple Protection Tubes make it a superior alternative to competitive tubes in temperature measurement, maintenance and product life areas.ApplicationsCrucibl.. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Ferro EG 2770 Specialty Glass Glass Type: Si-Al-Mg-Ca Typical Powder Form: TF Typical Application: Sintering Aid Ferro offers a wide range of compositions for specialty applications including sintering aids used in the glass-ph.. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Mateck Lithium Fluoride (LiF) Optical crystals |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Ferro EG 0002 Glazes and Sealants Glass Type: Si-Al-Ba Typical Powder Form: VWG Typical Application: SiC Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insulatin.. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Ferro EG 3600 Metal Sealing Glass Type: Si-Ba Alkali Typical Powder Form: VSD Typical Application: Compress.Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched se.. |
|||
Density | 2.60 - 3.20 g/cc | 0.0939 - 0.116 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 599.074 Agglomerated Sintered Molybdenum Carbide (Cr2O3) |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Schott G018-093 Dental Glass Remarks: Sr- and F-containing, low refractive glassApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provide.. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Schott GM31685 Dental Glass Remarks: Low refractive index glass ceramicApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provided by SCH.. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Schott GM32087 Dental Glass Remarks: Sr-containing, low refractive glassApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provided by SC.. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Schott GM35429 Dental Glass Remarks: High fluoride containing Ca-glassApplication: Glass ionomer cementAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provi.. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | ASTM D792 |
Saint-Gobain Rulon® 1439 Bearing/Seal PTFE Rulon® 1439 is a white FDA compliant material that is suitable for immersed service with better wear characteristics than most other PTFE compounds. Its color makes it aesthetically pleasing for .. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Sapco C 220 Steatite Information provided by Sapco. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | Fibre Density |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 37%/7781 Fiber Information provided by HexCel |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | Fibre Density |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 63%/120 E-Glass Fiber Information provided by HexCel |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | ASTM C20 |
CoorsTek Nitrogen Bonded Silicon Carbide, SCNB Thermal Shock Delta Tc = 400°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Du-Co Ceramics DC-16-L-3 Steatite Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Du-Co Ceramics DC-9-L-3 Steatite Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Corning Pyroceram® Glass Ceramic High strength, high elastic modulus, and uniform dielectric properties. Pyroceram® can be manufactured in ogival ( pointed arch) shapes, hemispheres, pressware sheets, and various machined shapes. .. |
|||
Density | 2.60 - 3.60 g/cc | 0.0939 - 0.130 lb/in³ | |
Alliance BIF-11 Bonded (Composite) Magnetic Material |
|||
Density | 2.60 - 3.60 g/cc | 0.0939 - 0.130 lb/in³ | |
Alliance BIF-17 Bonded (Composite) Magnetic Material |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon Thermabond® 99A60X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier.. |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon Thermabond® R37300X008 0.008" Uncured Silicone Rubber on Fiberglass Carrier Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction:Liner: 1 mil FEPProduct: Uncured Silicone RubberCarrier: 3 m.. |
|||
Density | 2.60 - 2.75 g/cc | 0.0939 - 0.0994 lb/in³ | |
3M Cool Roofing Granule (Wausau) 3M Cool Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products are designed specifically to have a higher total solar reflectance than standard granules... |
|||
Density | 2.60 - 3.60 g/cc | 0.0939 - 0.130 lb/in³ | |
Alliance BIF-16 Bonded (Composite) Magnetic Material |
|||
Density | 2.60 g/cc | 0.0939 lb/in³ | |
Schott BG28 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |