Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 15.4 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 15.4 - 15.8 g/cc
0.556 - 0.571 lb/in³
MarkeTech W80Cu Tungsten/Copper Heat Sink Material
WCu composites are made by vacuum infiltration of uniform controlled porous blocks of tungsten with molten copper. This results in a material with an interconnected Cu matrix that has high thermal c..
Density 15.4 g/cc
0.556 lb/in³
Indium Corp. Indalloy 184 Gold Solder Alloy
Information Provided by Indium Corporation
Density 15.4 g/cc
0.556 lb/in³
Wieland 1608 Wilaform Gold
Universally applicable yellow gold alloy.Applications: casting, chains, laminar decoration, pipes, tubingDental
Density 15.4 g/cc
0.556 lb/in³
Wieland Porta Maximum NF PFM Alloy
All-purpose alloy for low-fusing high expanding ceramicsApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneerin..
Copyright © lookpolymers.com All Rights Reserved