Polymer Property : Density = 1.352 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.352 g/cc

@Temperature 5.00 °C
0.04884 lb/in³

@Temperature 41.0 °F
Solvay Chemicals A50 Methylene chloride
Thanks to its specific characteristics, especially high solvent power, it is used where a high-grade economic solvent is required, because it successfully dissolves many organic compounds. Its high ..
Density 1.352 g/cc

@Temperature 5.00 °C
0.04884 lb/in³

@Temperature 41.0 °F
Solvay Chemicals E2000 Methylene chloride
Thanks to its specific characteristics, especially high solvent power, it is used where a high-grade economic solvent is required, because it successfully dissolves many organic compounds. Its high ..
Density 1.352 g/cc
0.04884 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP DF004RXP PC
LNP* Thermocomp* DF004RXP is a compound based on Polycarbonate resin containing 20% Glass Fiber. Some light color grades may have lower impact data than natural and black. Added features include: ..
Density 1.352 g/cc
0.04884 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP DF004RXP PC (Asia Pacific)
20% Glass Fiber Reinforced Polycarbonate. Some light color grades may have lower impact data than nature and black grade.