Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.25 g/cc | 0.0452 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® 503R PC (Europe-Africa-Middle East) LEXAN 503R is a medium viscosity, 10% glass reinforced, UV-stabilized, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance and exce.. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® HF500R PC (Europe-Africa-Middle East) LEXAN HF500R is an easy flow, 9% glass reinforced, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance and impact performance. |
|||
Density | 1.25 - 1.49 g/cc | 0.0452 - 0.0538 lb/in³ | Average value: 1.36 g/cc Grade Count:34 |
Overview of materials for PVC/Acrylic Alloy This property data is a summary of similar materials in the MatWeb database for the category "PVC/Acrylic Alloy". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Density | 1.25 - 1.28 g/cc @Temperature 250 - 270 °C |
0.0452 - 0.0462 lb/in³ @Temperature 482 - 518 °F |
Average value: 1.26 g/cc Grade Count:2 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ISO 2781 |
Huntsman AVALON® 98 AE Thermoplastic Polyurethane Introduction: AVALON 98 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 98 AE is part of the AVALON Perform Range and offers a premium soiling materi.. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ISO 1183 |
SABIC Innovative Plastics NORYL V01525 PPE+HIPS (Europe-Africa-Middle East) Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Ultem 1000RV PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ASTM D792 |
Techmer ES HiFill® HIPS GF30 30% Glass Filled Availability: North AmericaForms: PelletsGlass Fiber Reinforcement, 30% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON RE004 PA 66 LNP* STAT-KON* RE004 is a compound based on Nylon 66 resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp RF006Q PA 66 LNP* Thermocomp* RF006Q is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Reduced Moisture.This data was supplied by SABIC-IP for the Americas r.. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | |
Solvay Chemicals Sodium Hypochlorite Sodium hypochlorite in water solution is a yellow-greenish liquid with a pungent odor. Sodium hypochlorite is used as reagent, disinfectant, bleaching or oxidizing agent.EINECS Number: 231-668-3/CAS.. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ASTM D792 |
Lubrizol Stat-Rite® S-680 Static Control PETG Alloy Stat-Rite® S-680 is a static dissipative PETG alloy. Stat-Rite® M-680 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protectio.. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ASTM D792 |
Chase Plastics CP Pryme® PC310R Polycarbonate, 10% Glass Fiber Reinforced, Recycled Content Features: Good mold releaseRecycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | JIS K-6911 |
Unitika elitel UE3215 Polyester, Pellet Low molecular weight type UE3210UNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, paints, ink bin.. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | JIS K-6911 |
Unitika elitel UE3800 Polyester, Pellet Hot melt adhesives, Adhesives for polyvinylchlorideUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesiv.. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ISO 1183 |
CP-Polymer-Technik Wellamid® 6000 CF 18 HWCP 18% Carbon Fiber Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Density | 1.25 - 1.29 g/cc | 0.0452 - 0.0466 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 64 Flexible PVC, Sheathing Good flexibility at low temperatures |
|||
Density | 1.25 - 1.29 g/cc | 0.0452 - 0.0466 lb/in³ | ISO R 1183 |
Fainplast Compounds PHS 75/B Flexible PVC, Transparent Extrusion Pipes for gasoline CAVIS |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ASTM D792 |
Aclo Accutech Polypropylene Homopolymer HP0334W40L1 Wollastonite Reinforced |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | outer wall; ASTM D792 |
3M SMS Heat Shrink Tubing 3M Heat Shrink Tubing SMS is a co-extruded, dual wall product. It is a composite of a polyolefin shrinkable outer wall and a thermoplastic adhesive inner wall. SMS tubing does not degrade when expos.. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ASTM D792 |
Aclo Accutech Polypropylene Copolymer HP0335W40L Wollastonite Reinforced |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | STN 64 0111 |
Plastcom SLOVALEN PH 81 C 40 Polypropylene Homopolymer and Copolymer, 40% Micronized Talc FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 40% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 130°C... |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon R37732R079 0.079" (2.01 mm) Cured Silicone Rubber with FEP Film Substrate Design/Construction: Interleave: PolyethyleneSide 1: Cured Silicone RubberSubstrate: FEP FilmAppearance: Red silicone rubber chemically bonded to fluoropolymer filmThis data represents typical value.. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® HFD4271 PC (Europe-Africa-Middle East) Lexan* HFD4271 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4271 has enhanced mold release, impact ductility.. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ASTM D792 |
Adell RR-19 Polypropylene Copolymer; 43% Glass Reinforced, High Impact Data provided by Adell Plastics, Inc. |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ISO 1183 |
DuPont Performance Polymers Hytrel® 7246HS NC010 TPC-ET
(Unverified Data**) Hytrel® 7246HS NC010 is a high modulus, heat stabilized grade with nominal hardness of 72D.Information provided by DuPont |
|||
Density | 1.25 g/cc | 0.0452 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP DL002P PC LNP LUBRICOMP* DL002P is a compound based on Polycarbonate resin containing 10% PTFE. Added features of this material include: Exceptional Processing, Internally Lubricated. |