Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Network Polymers NPP 50-0753 Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Network Polymers NPP 50-2753 Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Petromont 1201 High Density Polyethylene Resin Petromont HDPE 1201 is a high-density polyethylene copolymer resin produced using the UNIPOL® Process. This resin is designed for use in the blow moulding of large parts such as multi-purpose shipp.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D4883 |
Chevron Phillips HiD® 9352 HDPE Natural Pipe Resin
(discontinued **) Resin Type: gas phase linear hexane copolymer; ASTM D3350 Classification 335520A; ASTM D4976 Classification: PE 235, A 55701Applications: corrugated pipe applicationsInformation provided by Chevron .. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D4883 |
Chevron Phillips HiD® 9354 HDPE Natural Pipe Resin
(discontinued **) Resin Type: gas phase linear hexane copolymerApplications: corrugated pipe applicationsInformation provided by Chevron Phillips Chemical Company. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ISO 1183 |
Total Finathene® 53140 HDPE, blow molding, sheet
(discontinued **) Finathene® 53140 is a high density polyethylene produced by the slurry loop low pressure polymerization process FINATHENE® 53140 has been especially developed for the manufacturing of blow molded .. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® LH5320 Injection Molding HDPE
(discontinued **) CopolymerApplications: Housewares, bowls, food containers, toysFormolene LH5320 is a high density polyethylene for injection molding applications.Meets all requirements of the U.S. Food and Drug Adm.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® LH5326 Injection Molding HDPE
(discontinued **) CopolymerApplications: Housewares, bowls, food containers, toysFormolene LH5326 is a high density polyethylene for injection molding applications.Meets all requirements of the U.S. Food and Drug Adm.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® HP5221 Pipe HDPE
(discontinued **) High Density Hexene Copolymer Formolene® HP5221 is a high performance copolymer that is designed for the most demanding requirements of corrugated pipe applications. Formolene® HP5221 meets the re.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® M5370PX High Density Polyethylene, Extrusion Grade ALATHON M5370PX is a copolymer with a narrow molecular weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processability. T.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® LR732011 High Density Polyethylene (Blow Molding Grade) ApplicationsThe PETROTHENE LR 7320 series of polyethylene resins exhibits an excellent balance of stiffness and environmental stress crack resistance. Typical applications include bottles for bleac.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® LR734001 High Density Polyethylene (Blow Molding Grade) ApplicationsThe PETROTHENE LR 7340 series of polyethylene resins exhibits good stiffness and ESCR. Typical applications include bottles for household chemicals.Regulatory StatusThe base resin LR 73.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® LR734001 High Density Polyethylene (Sheet & Profile Extrusion) ApplicationsThe PETROTHENE LR 7340 series of polyethylene resins exhibits good stiffness and ESCR. Typical applications include bottles for household chemicals.Regulatory StatusThe base resin LR 73.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
ICO Polymers ICOTEXâ„¢ 520-5004 1000 Micron EVA Powder Description: ICOTEX 520-5004 is an EVA powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and flexibility and a viny.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D4883 |
Ineos CP53-30 Polyethylene Copolymer CP53-30 is a high density polyethylene copolymer developed for corrugated piping applications. This product is recommended for use in applications that are required to meet AASHTO specifications M 2.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D4883 |
Ineos T50-500 HDPE Ineos T50-500 is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and en.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D4883 |
Ineos T50-500-171 Polyethylene Copolymer This is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use pro.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D4883 |
Ineos T50-800 HDPE T50-800 is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use .. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D4883 |
Ineos T50-800-01 Polyethylene Copolymer This is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use pro.. |
|||
Density | 0.953 - 0.959 g/cc | 0.0344 - 0.0346 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GF 4950 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.953 - 0.961 g/cc | 0.0344 - 0.0347 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GM 5240 PR HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® M5350 High Density Polyethylene ApplicationsALATHON M 5350 copolymer with narrow molecular weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processing s.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ISO 1872/1 |
SIDPEC EGYPTENE® HD 5226 EA HDPE Injection Molding Applications:House waresThin-walled food containersPET bottle base cupInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ISO 1872/1 |
SIDPEC EGYPTENE® HD 5301 FB HDPE Film Applications:Strong thin filmCarrier bagGrocery sacksFilm properties were measured on 15 micron film extruded at a blow up ratio of 5:1, 8D neck height.Information provided by Interchim s.r.l., offi.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ISO 1183 |
Borealis BorSafe™ HE3495-LS HDPE Compound BorSafe™ HE3495-LS is a bimodal polyethylene compound produced by the advanced Borstar® technology. It's fully stabilized against thermal degradation and the die build-up during extrusion is minim.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® E922 Film HDPE High Density Polyethylene Medium Molecular Weight Bi-Modal Resin Designed for Film Applications Formolene® E922 is a medium molecular weight grade of HDPE designed for good processing characteristi.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ExxonMobil Method |
ExxonMobil Escorene® UL 8705 Adhesive Application Resin Escorene Ultra UL 8705 is a relatively low viscosity, 27.6% vinyl acetate copolymer specifically tailored for enhanced modulus/tensile performance at the same viscosity of similar materials. It has .. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | |
Dow HDPE 65053N High Density Polyethylene DOW HDPE 65053N resin is a narrow molecular weight distribution copolymer designed to offer good environmental stress crack resistance and rigidity with high impact strength. This resin has excellen.. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D1505 |
Amco PRIMATOP HDPE 175953 Injection Molding Polyethylene HDPE 175953 features easy flow, toughness, and high surface gloss. Applications include caps, thin wall parts, and toys.Former A-Top Polymers product; part of Amco product line since 2013. |
|||
Density | 0.953 g/cc | 0.0344 lb/in³ | ASTM D4883 |
Ineos J50-2000-119 HDPE HDPE J50-2000-119 is a high density, narrow molecular weight polyethylene copolymer intended for applications requiring a glossy surface finish and reasonably good impact strength and rigidity. It i.. |