Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.941 g/cc | 0.0340 lb/in³ | ASTM D 792 |
NOVA Chemicals Surpass® RMs341-U Octene sHDPE Rotational Molding Resin RMs341-U complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. RMs341-.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | Exxon Method |
ExxonMobil Escor® AT-310 EMAAA Terpolymer for Polymer Modification
(discontinued **) Data provided by the manufacturer, Exxon Chemical.45 Acid Number. Provides unusual adhesion to a variety of substrates and other components such as aluminum foil, polyolefins, polycarbonate, PET, e.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® CL-200YJN (Natural) Rotational molding crosslinkable high density polyethylene
(disc Benefits: crosslinks during molding - has outstanding melt strength at 204°C, is formulated to provide maximum UV protection for long-term outdoor weathering, contains an internal mold release, exc.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® CL-200YNR JN (Natural) Rotational molding crosslinkable high density polyethylene
(d Benefits: crosslinks during molding - has outstanding melt strength at 204°C, is formulated to provide maximum UV protection for long-term outdoor weathering, contains an internal mold release, exc.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ASTM D792-ISO 1183 |
DuPont Elvax® 466 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 466 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications:Elvax® 466 resins can be used for the following applications: adhesives, sealants.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ExxonMobil Method |
ExxonMobil Escorene® LD 720.92 Specialty Film Resin
(discontinued **) Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and tou.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ExxonMobil Method |
ExxonMobil Escorene® UL 7620 Adhesive Application Resin
(discontinued **) Escorene Ultra UL 7620 is a medium flow rate, 24% vinyl acetate copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt adhesives, s.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-720 High EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer specialty film resin designed for applications requiring outstanding heat sealability along with excellent strength p.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ASTM D 792 |
NOVA Chemicals Surpass® RMs341-UG Octene sHDPE Rotational Molding Resin RMs341-UG complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. RMs341.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 2515 MDPE Injection Molding Resin
(discontinued **) Features: Excellent processability for applications requiring moderate stiffness and improved toughnessExcellent cold temperature impact properties Applications: Ice cream containersHousewares Deep.. |
|||
Density | 0.941 - 0.947 g/cc | 0.0340 - 0.0342 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GM 7746 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.941 - 0.983 g/cc | 0.0340 - 0.0355 lb/in³ | |
Lord Adhesives Flocklok® 850 Flock Adhesive Flocklok® 850 is a moisture curing, polyurethane flock adhesive. It is used to adhere flock to SBR elastomers, thermoplastic elastomers, and plastics (i.e., ABS). Thermoplastic elastomers will re.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | |
Lord Adhesives Flocklok® 851 Flock Adhesive Flocklok® 851 is a moisture curing, polyurethane flock adhesive used to adhere flock to SBR, thermoplastic elastomers, and plastic (i.e., ABS). Thermoplastic elastomers will require the use of a .. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | Mixed |
ITW Plexus Plexusâ„¢ MA3940 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Use with craze sensitive plastics.Information provided by Illinois Tool Works. |
|||
Density | 0.941 - 0.947 g/cc | 0.0340 - 0.0342 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GM 7746 A HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | LE 4437; ASTM D792 |
Borealis Visico™ LE4421/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation Visico LE4421/LE4437 is a natural, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination of a Visico base materi.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ASTM D 792 |
Total 3802 Blue MDPE pipe, injection molding FINATHENE® 3802 Blue is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Blue is a blue polyeth.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ASTM-D1505 |
Westlake EMAC® Plus SP1501 20% EMA Copolymer Westlake EMAC� Plus SP1501 is a 20% EMA copolymer designed for extrusion coating, compounding, and blending where low viscosity, flexibility, and strength are important. SP1501 provides excelle.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ASTM D1505 |
Westlake EMAC® SP2220 20% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2220 is a 20% EMA copolymer designed for compounding, extrusion coating, tie-layers, and extrusions where flexibility, compatibility, low heat seal temperatures, or high coefficien.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ASTM-D1505 |
Westlake EMAC® SP2404 18.5% EMA Copolymer Westlake EMAC� SP2404 is a 18.5% EMA copolymer designed for blown film, tie-layer, coextrusions, and blending where flexibility and strength are important. SP2404 provides excellent elasticity .. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ASTM-D1505 |
Westlake EMAC® SP2409 20% EMA Copolymer Westlake EMAC� SP2409 is a 20% EMA copolymer designed for extrusion coating, tie-layers, and extrusions where flexibility, compatibility, low heat seal temperatures, or a high coefficient of fr.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ISO 1183 |
Borealis CG8410 High Density Polyethylene CG8410 is a high-density polyethylene for extrusion coating. Applications: extrusion coating of high volume production of boards and papers.Information provided by Borealis AG |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ UL 00218CC3 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00218CC3 is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperature above 240°C (464°F) may cause resin degradation.Availability: Africa & M.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ UL 7711 Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 7711 is a very high flow, 26.7% VA copolymer that has very good compatibility with hydrocarbon and natural tackifiers and most waxes. It is suitable for making.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Appeel® 20D867 Ethylene Acrylate DuPont™ Appeel 20D867 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ExxonMobil Method |
ExxonMobil Escorene® LD 720.01 Specialty Film Resin Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and tou.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ FL 00218 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00218 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 240°C (464°F) may cause resin degradation. Machines should always b.. |
|||
Density | 0.941 g/cc | 0.0340 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 2508-UV13 MDPE Injection Molding Resin