Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.938 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Polimeros Mexicanos Rotolene® Industrial Black Linear Medium Density Polyethylene Hexene Copolymer Linear Medium Density Polyethylene grade which is fully UV8 stabilized. High quality Polyethylene compounded in black, formulated for rotational molding applications requiring excel.. |
|||
Density | 0.938 - 0.942 g/cc | 0.0339 - 0.0340 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4440R (40404) Medium Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® TD-9055-E Hexene LMDPE Film Resin Excellent stiffness and glossApplications: Diaper back sheet, BlendingAdditives: High temperature AOFilm properties are typical of cast film extruded at 280°C.Information provided by NOVA Chemicals.. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® TF-0338-E Hexene LMDPE Film Resin Excellent stiffness and glossApplications: Diaper back sheet, BlendingAdditives: High temperature AOFilm properties are typical of film extruded at 280°C.Information provided by NOVA Chemicals. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ASTM D 792 |
NOVA Chemicals Novapol® TF-0438-E Hexene LMDPE Film Resin TF-0438-E complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatur.. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ASTM D4883 |
ExxonMobil Escorene® LL-8461 LLDPE, Rotational Molding Powder
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated, UV-8 type protection, Good stiffnessUses: Septic tanks, Chemical storage bins, Potable water tanks |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | Exxon Method |
ExxonMobil Escorene® LL-8461 LMDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.LL-8400 series are linear medium density polyethylene resins that provide outstanding environmental stress crack resistance. LL-8461 is fully formu.. |
|||
Density | 0.938 - 1.01 g/cc | 0.0339 - 0.0365 lb/in³ | Average value: 0.954 g/cc Grade Count:266 |
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum.. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | |
LyondellBasell Lupolen® 3822 D GB 00350 MDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ASTM D1505 |
ICO Polymers ICORENEâ„¢ 115-1653 LMDPE Rotational Molding Resin Description: ICORENE 115-1653 polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and generally balanced physical pro.. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ASTM D792 |
Micropol Microlin ML90 Linear Polyethylene Rotational Molding Powder Information provided by Micropol Limited |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ASTM 1505-68 |
Iran Petrochemical (PCC) 3840 UA Medium Density Polyethylene MD3840UA is a linear medium density polyethylene (MDPE) with butene copolymer. This polymer has good impact strength, excellent external and internal surface finish, whiteness, good stress cracking .. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ISO 1872/1 |
SIDPEC EGYPTENE® HD 3840 EA MDPE Wire and Cable Grade Applications:Suitable for the production of silane cross-linkable compoundsLow voltage power cable insulationInjection molded technical parts and closureInformation provided by Interchim s.r.l., off.. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ISO 1872/1 |
SIDPEC EGYPTENE® HD 3840 UA MDPE Rotational Molding Applications:Rotational items: tanks, containers, etc...Injection molded technical parts and closureInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (S.. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ISO 1183 |
Unipetrol PE HD LITEN® FB/FL 20 HDPE Made for tubular film and special applications.Information provided by Unipetrol RPA |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® HL3812 Film (Hexene) HDPE Medium Density Polyethylene Formolene® HL3812 is a high molecular weight hexene copolymer resin that is tailored specifically for geomembrane applications. The resin provides an excellent balance o.. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ASTM D792 |
DuPont Bynel® 3930 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ASTM D 792 |
Total HT 514 MDPE film Finathene® HT 514 is a medium density polyethylene produced by the slurry loop low pressure polymerization process. Finathene® HT 514 can be used alone, blended or coextruded in a wide variety of .. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ASTM D4883 |
ExxonMobil LL 8460.29 Rotational Molding Resin Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o.. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ExxonMobil method |
ExxonMobil LLDPE LLP 8460.29 Linear Low Density Polyethylene Resin Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o.. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ASTM D4883 |
ExxonMobil LLP8460.29 Rotational Molding Resin Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o.. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | |
Dow Primacor® 1430 Ethylene Acrylic Acid (EAA) Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ExxonMobil Method |
ExxonMobil Escorene® UL 7520 Adhesive Application Resin Escorene Ultra UL 7520 is a high flow, 18.5% vinyl acetate copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt adhesives, sealan.. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ FL 01418 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 01418 is primarily designed for high speed/low coating weight extrusion coating and is a good coextrusion partner with other polymers. FL 01418 is an excellent sealing materi.. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | |
Dow Primacor® 1410 Ethylene Acrylic Acid (EAA) Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | |
Dow Primacor® 3440 Ethylene Acrylic Acid (EAA) PRIMACOR® 3440 polymer containing 9.5% comonomer is an extrusion/ coextrusion coating and laminating for flexible packaging applications. It is designed to provide excellent hot tack and adhesion t.. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® TR-0338-UG MDPE Rotational Molding Resin
(discontinued **) Molded Plaque Properties. Features: Hexene Copolymer, excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer. |
|||
Density | 0.938 g/cc | 0.0339 lb/in³ | ASTM D4883 |
ExxonMobil LL 8460 Rotational Molding Resin
(discontinued **) LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require optimum balance of stiffness, processabili.. |