Material Notes:
Escorene Ultra UL 7520 is a high flow, 18.5% vinyl acetate copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt adhesives, sealants and wax blends.Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Applications:Adhesives and SealantsHot Melt AdhesivesIndustrial SealantsWax Blends Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.938 g/cc
0.0339 lb/in³
ExxonMobil Method
Vinyl Acetate Content 18.5 %
18.5 %
ExxonMobil Method
Melt Flow 140 g/10 min

@Load 2.16 kg,
Temperature 190 °C
140 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 82
82
15s; ASTM D2240
Hardness, Shore D 26
26
15s; ASTM D2240
Tensile Strength at Break 4.21 MPa
610 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 0.0414 GPa
6.00 ksi
1% secant; ASTM D790
Thermal Properties Metric English Comments
Melting Point 82.8 °C
181 °F
Peak Melting Temperature; ExxonMobil Method
Vicat Softening Point 47.2 °C
117 °F
ASTM D1525
Descriptive Properties Value Comments
Features Thermal Stabilizer