Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D792 |
Polimeros Mexicanos Rotolene® Black Plus Polyethylene Polyethylene compound specially formulated for rotational molding applications requiring good mechanical properties and good mold release properties. Rotational molded parts have smooth surface and .. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ExxonMobil Method |
ExxonMobil OPTEMA™ TC 115 Molding, extrusion and compounding resin
(discontinued **) OPTEMA TC 115 is an ethylene methyl acrylate copolymer, which can be used as a compatibilizer and impact modifier for engineering thermoplastics. It has been processed at temperatures up to 625°F w.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D4883 |
ExxonMobil LL 8450 Rotational Molding Resin
(discontinued **) LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. This resin is ideally suited for applications that require optimum balance.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D 792 |
Total Finathene® DF 210 HDPE resin
(discontinued **) Applications: Irrigation tape and tubingInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | Exxon Method |
ExxonMobil Escorene® MV-02528 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 27.5% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® HL3721 Sheet and Thermoforming HDPE
(discontinued **) Medium Density Hexene CopolymerApplications: Geomembranes, gas and chemical tank containment liners, landfill liners.Formolene HL3721 is tailored for extrusion applications requiring good processabi.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® HL3712 Sheet and Thermoforming HDPE
(discontinued **) Medium Density Hexene CopolymerApplications: Gas and chemical tank containment liners, pond liners, landfill liners, tunnel liners.Formolene HL3712 has good processability, excellent melt strength, .. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Braskem LH 437 LMDPE Cast Film Extrusion Polyethylene
(discontinued **) Applications: Diapers (back sheet); Absorbent pads (back sheet). Information provided by Braskem |
|||
Density | 0.937 - 0.945 g/cc | 0.0339 - 0.0341 lb/in³ | |
Kazanorgsintez 298-285 High Density Polyethylene Composite Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions 296-.. |
|||
Density | 0.937 - 0.945 g/cc | 0.0339 - 0.0341 lb/in³ | |
Kazanorgsintez 298-285D High Density Polyethylene Composite Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions 296-.. |
|||
Density | 0.937 - 0.943 g/cc | 0.0339 - 0.0341 lb/in³ | |
Kazanorgsintez PE80B-285 High Density Polyethylene Composite, Film Grade Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions are .. |
|||
Density | 0.937 - 0.943 g/cc | 0.0339 - 0.0341 lb/in³ | |
Kazanorgsintez PE80B-285D High Density Polyethylene Composite, Film Grade Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions are .. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D4883 (Natural) |
Ineos G36-10-150 HDPE G36-10-150 is a medium density hexene copolymer polyethylene resin designed for the blown geomembrane sheet process. This resin is especially well suited for the production of textured geomembranes... |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D4883 |
Ineos G36-24-150 HDPE Ineos G36-24-150 is a medium density polyethylene resin designed for geomembrane sheet extrusion. The resin has excellent environmental stress crack resistance (ESCR).Natural resin; some physical p.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) MF3713 High Density Polyethylene MF3713 is a high molecular weight high density polyethylene.Applications: bags, products for use in property modification.Information provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | compound; ISO 1872-2/ISO 1183 |
Borealis Borcell™ ME1244 Medium Density Polyethylene Borcell™ ME1244 is a fully formulated compound for chemical foamed telesingles. ME1244 is a medium-density polyethylene compound containing chemical blowing agent. Applications Borcell™ ME1244 i.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D792-ISO 1183 |
DuPont Elvax® 420 Ethylene Vinyl Acetate DuPont™ Elvax® 420 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications:Elvax® 420 resins can be used for the following applications: adhesives, sealants.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ISO 1183 |
Total MDPE HL 323 Medium Density Polyethylene, Film Resin Medium molecular weight, medium density film resinCharacteristics:Excellent balance of stiffness and impact strengthGood puncture resistanceExcellent compatibility with LDPE and LLDPEGood tensile st.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® HF3728 Film (Hexene) HDPE High Density Polyethylene Medium Molecular weight Film Resin Formolene® HF3728 is a medium density resin that provides an excellent overall balance of tensile, impact, and tear properties in thin f.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Chevron Phillips MarFlex® HHM TR-130 MDPE Film Resin Medium density resin provides overall balance of tensile, impact, and tear properties in film. It is suited for merchandise, produce, and trash bags. Processing performance is excellent on high st.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ FL 00014 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00014 is a copolymer of ethylene and vinyl acetate. For film requiring very high toughness, low creep, excellent optical properties and low gel.Availability: Africa & Middle .. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ UL 00014 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00014 is a fractional MI copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applic.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ UL 53019CC Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 53019CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agent.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ExxonMobil method |
ExxonMobil LLDPE LLP 8450.31 Linear Low Density Polyethylene Resin Product Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that require.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D4883 |
ExxonMobil LLP8450.31 Rotational Molding Resin LProduct Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that requir.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ISO 1183 |
Borealis Borstar® FB4370 Medium Density Polyethylene Borstar® FB4370 is a linear medium density polyethylene grade combining excellent extrusion properties with high film stiffness. Applications: Borstar® FB4370 has been developed especially for ap.. |