Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.885 g/cc @Temperature 15.6 °C |
0.0320 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil 80 Exxon Aviation Oil EE Series Aviation Oil EE is the brand name of a premium quality line of ashless-dispersant piston engine oils. Formulated with select, highly refined base oils together with ashless-dispersant and anti-oxida.. |
|||
Density | 0.885 g/cc @Temperature 15.0 °C |
0.0320 lb/in³ @Temperature 59.0 °F |
ASTM D1298 |
ExxonMobil Mobil Pegasus 701 Series 40 Mobil Pegasus 701 Series are premium natural gas engine oils formulated exclusively from specially selected base stocks of high stability. These lubricants provide the excellent performance and econ.. |
|||
Density | 0.885 g/cc | 0.0320 lb/in³ | ASTM D792 |
Dow AFFINITY™ EG 8185 Polyolefin Plastomer (POP) AFFINITY™ EG 8185 Polyolefin Plastomer (POP) is produced via INSITE™ Technology. It is a lower density POP polymer exhibiting high elasticity for fibers.Information provided by Dow |
|||
Density | 0.885 g/cc | 0.0320 lb/in³ | |
Dow AFFINITY™ SM 8250 Polyolefin Plastomer AFFINITY® SM 8250 polyolefin plastomer is an alpha-olefin resin that offers excellent performance in injection molded clear or colored flexible durable parts. It exhibits excellent clarity and flex.. |
|||
Density | 0.885 g/cc | 0.0320 lb/in³ | |
Dow AFFINITY™ VP 8770 Polyolefin Plastomer AFFINITY® VP 8770 polyolefin plastomer is an alpha-olefin resin for general purpose applications. It exhibits excellent optics and flexibility. Its low specific gravity can help control resin and p.. |
|||
Density | 0.885 g/cc @Temperature 15.6 °C |
0.0320 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil 80 Exxon Aviation Oil EE Series Aviation Oil EE is the brand name of a premium quality line of ashless-dispersant piston engine oils. Formulated with select, highly refined base oils together with ashless-dispersant and anti-oxida.. |
|||
Density | 0.885 g/cc | 0.0320 lb/in³ | ASTM D792 |
Dow Engage® 8003 Polyolefin Elastomer Description: Engage® 8003 polyolefin elastomer is an ethyleneoctene copolymer that has excellent flow characteristics and performs well in a wide variety of general purpose thermoplastic elastomer .. |
|||
Density | 0.885 g/cc | 0.0320 lb/in³ | ASTM D792 |
Dow Engage® 8401 Polyolefin Elastomer Description: Engage® 8401 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in durable, flexible injection molded industrial and consumer goods. Engage® 8401 pr.. |
|||
Density | 0.885 g/cc | 0.0320 lb/in³ | ASTM D792 |
Dow Engage® ENR 7256.00 Ethylene-Butene Copolymer Description: ENR 7256.00 is a unique broader molecular weight distribution ethylene-butene copolymer with higher branching levels that offers excellent clarity, processing and performance in foams a.. |
|||
Density | 0.885 g/cc @Temperature 15.0 °C |
0.0320 lb/in³ @Temperature 59.0 °F |
ASTM D1298 |
ExxonMobil Mobil Pegasus 701 Series 40 Mobil Pegasus 701 Series are premium natural gas engine oils formulated exclusively from specially selected base stocks of high stability. These lubricants provide the excellent performance and econ.. |
|||
Density | 0.885 g/cc @Temperature 23.0 °C |
0.0320 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Arkema Group OREVAC® 18390 Maleic Anhydride Modified Polyethylene OREVAC® 18390 is anhydride modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 1.. |
|||
Density | 0.885 g/cc | 0.0320 lb/in³ | ASTM D1505 |
M. Holland Company MAGMA® LM311-D LLDPE
(discontinued **) Features: Good Processability, Good Puncture Resistance, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |