Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.884 - 2.12 g/cc | 0.0319 - 0.0766 lb/in³ | Average value: 1.05 g/cc Grade Count:383 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Density | 0.884 g/cc @Temperature 20.0 °C |
0.0319 lb/in³ @Temperature 68.0 °F |
|
LyondellBasell PNP Propylene glycol normal propyl ether Information provided by Lyondell. |
|||
Density | 0.884 g/cc @Temperature 15.0 °C |
0.0319 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 16M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Density | 0.884 g/cc @Temperature 15.0 °C |
0.0319 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 68 Mobil EAL Envirosyn H Series Mobil EAL Envirosyn H Series oils are super premium, high performance fully synthetic environmentally aware hydraulic and circulating oils designed to provide outstanding performance in systems oper.. |
|||
Density | 0.884 g/cc @Temperature 15.0 °C |
0.0319 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Nuto 100 H Series Exxon Nuto H Series oils are premium quality anti-wear hydraulic oils intended for industrial and mobile service applications where anti-wear lubricants are required. They are formulated with high q.. |
|||
Density | 0.884 g/cc | 0.0319 lb/in³ | ASTM D792 |
Dow FLEXOMER™ DFDB-1088 NT Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ DFDB-1088 NT is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It can be utilized in monolayer and co-extruded films and in blends with other polyolefins to.. |
|||
Density | 0.884 g/cc | 0.0319 lb/in³ | ASTM D792 |
Dow FLEXOMER™ GERS-1088 NT Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ GERS-1088 NT is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It can be utilized in monolayer and co-extruded films and in blends with other polyolefins to.. |
|||
Density | 0.884 g/cc @Temperature 15.0 °C |
0.0319 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Nuto 100 H Series Exxon Nuto H Series oils are premium quality anti-wear hydraulic oils intended for industrial and mobile service applications where anti-wear lubricants are required. They are formulated with high q.. |
|||
Density | 0.884 g/cc | 0.0319 lb/in³ | |
ConocoPhillips Conoco® El Mar® Grade 30 Mid Ash Supreme Oil Conoco® El Mar Mid Ash Supreme is a premium quality, mid-ash, dispersant-detergent gas engine oil designed for use in naturally aspirated and moderately to highly turbocharged 4-stroke cycle natura.. |
|||
Density | 0.884 g/cc | 0.0319 lb/in³ | |
ConocoPhillips Hydroclear® 150 Rock Oil Description: Conoco Hydroclear Rock Drill Oil is a high-quality, heavy-duty, extreme-pressure pneumatic tool lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Rock Drill .. |
|||
Density | 0.884 g/cc | 0.0319 lb/in³ | |
ConocoPhillips Hydroclear® 220 TCS Slideway lubricant Description: Conoco Hydroclear® TCS Slideway Lubricant is a premium demulsible machine tool way lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear TCS Slideway Lubricant .. |
|||
Density | 0.884 g/cc @Temperature 15.0 °C |
0.0319 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 16M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Density | 0.884 g/cc @Temperature 15.0 °C |
0.0319 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 68 Mobil EAL Envirosyn H Series Mobil EAL Envirosyn H Series oils are super premium, high performance fully synthetic environmentally aware hydraulic and circulating oils designed to provide outstanding performance in systems oper.. |