Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.882 g/cc | 0.0319 lb/in³ | ASTM D792 |
LyondellBasell Adflexâ„¢ Q 200 F Polyolefin Description: Adflexâ„¢ Q 200 F fractional melt flow, low modulus thermoplastic olefin (TPO) resin is designed for extrusion applications. It is based on material produced from Basell's propri.. |
|||
Density | 0.882 g/cc | 0.0319 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Polidiemme® G/440 Thermoset Elastomer (TSE) Elastomer based compound crosslinkable by ambient moisture, consisting of a silane pregrafted base compound to be used with a catalyst masterbatch (Sioplas® method)Standards complying: Cenelec HD.. |
|||
Density | 0.882 g/cc @Temperature 15.0 °C |
0.0319 lb/in³ @Temperature 59.0 °F |
|
ExxonMobil 100 Exxon Sawguide Oil EXXON SAWGUIDE OIL is specifically formulated to lubricate the thin saw blades of modern gang saws and edgers. The choice of viscosity grade depends on equipment type, lubricant delivery system desi.. |
|||
Density | 0.882 g/cc @Temperature 15.6 °C |
0.0319 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil 20W-50 Exxon Aviation Oil Aviation Oil 100, 120 and 20W-50 are non-dispersant, mineral oil-based lubricants for piston engines of commercial, military and private aircraft. They contain very low concentrations of anti-oxid.. |
|||
Density | 0.882 g/cc @Temperature 15.6 °C |
0.0319 lb/in³ @Temperature 60.1 °F |
|
ExxonMobil Mobilarma 524 Mobilarma 500 Series oils are premium performance products primarily intended as run-in or lay-up lubricants, which provide effective rust preventive films on the internal surfaces of machinery. The.. |
|||
Density | 0.882 g/cc | 0.0319 lb/in³ | ISO 1183 |
ExxonMobil EXACT™ 8210 Plastomer for Multilayer Film Applications Product Description: Exact 8210 plastomer is an ethylene octene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology. It is designed for seal layers in multilayer film applications req.. |
|||
Density | 0.882 g/cc | 0.0319 lb/in³ | ISO 1183 |
ExxonMobil EXACT™ 8230 Plastomer for Polymer Modification Product Description: Exact 8230 plastomer is an ethylene octene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties. It is designed.. |
|||
Density | 0.882 g/cc @Temperature 15.6 °C |
0.0319 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil 20W-50 Exxon Aviation Oil Aviation Oil 100, 120 and 20W-50 are non-dispersant, mineral oil-based lubricants for piston engines of commercial, military and private aircraft. They contain very low concentrations of anti-oxid.. |
|||
Density | 0.882 g/cc @Temperature 15.6 °C |
0.0319 lb/in³ @Temperature 60.1 °F |
|
ExxonMobil Mobilarma 524 Mobilarma 500 Series oils are premium performance products primarily intended as run-in or lay-up lubricants, which provide effective rust preventive films on the internal surfaces of machinery. The.. |
|||
Density | 0.882 g/cc @Temperature 15.6 °C |
0.0319 lb/in³ @Temperature 60.1 °F |
|
ExxonMobil Mobilarma 798 The Mobilarma 700 Series contains three premium performance rust preventives that cover a range of applications including storage and inter-operational activities. The Mobilarma 777 and 778 are inte.. |
|||
Density | 0.882 g/cc @Temperature 15.0 °C |
0.0319 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobiltrans AST Mobiltrans AST (All Season Transmission) is an extra high performance drivetrain lubricant engineered to meet Caterpillars new TO-4 performance specifications for off-highway transmissions, drive tr.. |
|||
Density | 0.882 g/cc @Temperature 15.0 °C |
0.0319 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Nuto 68 H Series Exxon Nuto H Series oils are premium quality anti-wear hydraulic oils intended for industrial and mobile service applications where anti-wear lubricants are required. They are formulated with high q.. |
|||
Density | 0.882 g/cc | 0.0319 lb/in³ | |
ConocoPhillips Conoco® El Mar® 2000 Oil SAE Grade 30 Conoco® El Mar 2000 is a high-quality, very low-ash, dispersant detergent gas engine oil designed for use in naturally aspirated and moderately turbocharged, low- to medium-speed 2-stroke cycle and.. |
|||
Density | 0.882 g/cc | 0.0319 lb/in³ | |
ConocoPhillips Conoco® El Mar® Ashless Heavy Duty Oil, SAE Viscosity Grade 30 Conoco® El Mar Ashless Heavy Duty is a high-quality, ashless, dispersant-detergent gas engine oil designed for use in naturally aspirated and moderately turbocharged 2-stroke cycle natural gas engi.. |
|||
Density | 0.882 g/cc | 0.0319 lb/in³ | |
ConocoPhillips El Mar® 3000 Oil SAE Grade 30 Description: Conoco El Mar® 3000 Oil is a quality, low ash gas engine oil recommended for naturally aspirated and moderately turbocharged, four cycle, low-, medium- and high-speed gas engines, such.. |
|||
Density | 0.882 g/cc | 0.0319 lb/in³ | |
ConocoPhillips El Mar® 3000 Oil SAE Grade 40 Description: Conoco El Mar® 3000 Oil is a quality, low ash gas engine oil recommended for naturally aspirated and moderately turbocharged, four cycle, low-, medium- and high-speed gas engines, such.. |
|||
Density | 0.882 g/cc | 0.0319 lb/in³ | |
ConocoPhillips Hydroclear® 68 Multi-Way Machine Lubricant Description: Conoco Hydroclear Multi-Way Machine Lubricant is a high-quality, heavy-duty circulating machine tool lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Multi-.. |
|||
Density | 0.882 g/cc | 0.0319 lb/in³ | |
ConocoPhillips Hydroclear® El Mar® Ashless Heavy Duty SAE 30 Description: Conoco Hydroclear El Mar Ashless Heavy Duty is a high-quality, ashless natural gas engine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear El Mar Ashless Heavy D.. |
|||
Density | 0.882 g/cc @Temperature 15.0 °C |
0.0319 lb/in³ @Temperature 59.0 °F |
|
ExxonMobil 100 Exxon Sawguide Oil EXXON SAWGUIDE OIL is specifically formulated to lubricate the thin saw blades of modern gang saws and edgers. The choice of viscosity grade depends on equipment type, lubricant delivery system desi.. |
|||
Density | 0.882 g/cc @Temperature 15.0 °C |
0.0319 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobiltrans AST Mobiltrans AST (All Season Transmission) is an extra high performance drivetrain lubricant engineered to meet Caterpillars new TO-4 performance specifications for off-highway transmissions, drive tr.. |
|||
Density | 0.882 g/cc @Temperature 15.0 °C |
0.0319 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Nuto 68 H Series Exxon Nuto H Series oils are premium quality anti-wear hydraulic oils intended for industrial and mobile service applications where anti-wear lubricants are required. They are formulated with high q.. |
|||
Density | 0.882 g/cc | 0.0319 lb/in³ | |
BASF 2-Ethylhexanal Formula: C8H16OCAS: 123-05-7Description: 2-Ethylhexanal is a colorless to yellow liquid, with a characteristic odor. It is partially miscible with water.Applications: Intermediate used in chemical .. |
|||
Density | 0.882 - 3.50 g/cc | 0.0319 - 0.126 lb/in³ | Average value: 1.06 g/cc Grade Count:387 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma.. |
|||
Density | 0.882 g/cc | 0.0319 lb/in³ | |
ConocoPhillips Conoco® El Mar® Ashless Supreme Oil, SAE Viscosity Grade 30 Conoco® El Mar Ashless Supreme is a premium quality, ashless, dispersant-detergent gas engine oil designed for use in naturally aspirated and turbocharged 2-stroke cycle natural gas engines. Engine.. |
|||
Density | 0.882 g/cc @Temperature 15.6 °C |
0.0319 lb/in³ @Temperature 60.1 °F |
|
ExxonMobil Mobilarma 798 The Mobilarma 700 Series contains three premium performance rust preventives that cover a range of applications including storage and inter-operational activities. The Mobilarma 777 and 778 are inte.. |