Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.870 - 11.0 g/cc | 0.0314 - 0.397 lb/in³ | Average value: 1.06 g/cc Grade Count:952 |
Overview of materials for Styrenic Elastomer (TES) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro.. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | ASTM D1505 |
M. Holland Company MAGMA® LM372-A LLDPE
(discontinued **) Features: High Clarity, Good Flexibility, Good Flow, High Gloss, Good ToughnessProcessing Method: Injection MoldingInformation provided by M. Holland. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | d20/20 |
Mitsui UNISTOLEâ„¢ P-401AM Polyolefinic Primer/ Adhesive UNISTOLEâ„¢ P is a liquid primer for coating and bonding polypropylene (PP) and various engineering plastics, rubber and other materials, which do not readily bond. Characteristics An easily han.. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | |
Solvay MACKINE® 401 Surfactant Product Description: Mackine 401 is slightly soluble in water but becomes readily soluble when neutralized with acid, becoming a cationic surfactant. The tertiary amine group can also react with hyd.. |
|||
Density | 0.870 g/cc @Temperature 15.6 °C |
0.0314 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil 220 Mobilgear SHC Series The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol.. |
|||
Density | 0.870 g/cc @Temperature 15.0 °C |
0.0314 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil Delvac 80W-140 Synthetic Gear Oil Mobil Delvac Synthetic Gear Oil 75W-90 and 80W-140 are synthetic drivetrain lubricants engineered to meet the most demanding extended drain and warranty requirements. These products are designed for.. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Fusabond® N493 Polymer Modifier DuPont™ Fusabond® N493 is an anhydride modified ethylene copolymer. DuPont™ Fusabond® N493 can only be used in the following applications: all polyamide blends and blends for golf balls and ble.. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | |
DuPont™ Nomex® 410 Paper, 5 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Density | 0.870 g/cc @Temperature 15.0 °C |
0.0314 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 15W-40 Exxon XD-3 Elite Exxon XD-3 15W-40 is a synthetic blend heavy duty diesel engine oil that provides the highest level of protection to modern, high performance diesel engines used in severe on and off highway applic.. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | |
Dow AFFINITY™ EG 8100 Polyolefin Elastomer AFFINITY® EG 8100 polyolefin elastomer is a saturated ethylene-octene copolymer for general purpose elastomeric applications that is efficiently crosslinked by peroxide, silane or irradiation It ex.. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | ASTM D792 |
Dow AFFINITY™ EG 8100G Ethylene-octene copolymer AFFINITY™ EG 8100G Polyolefin Plastomer (POP) is produced via INSITE™ Technology. It is a general purpose ethylene-octene copolymer exhibiting high flexibility and elasticity. It can be utilized.. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | ASTM D792 |
Dow AFFINITY™ GA 1900 Polyolefin Plastomer (POP) AFFINITY™ GA 1900 Polyolefin Plastomer (POP) is produced via INSITE™ Technology from Dow Plastics. This product can be used in applications such as polymer modification (i.e. flow enhancement and.. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | ASTM D792 |
Dow Engage® 8207 Polyolefin Elastomer Description: Engage® 8207 polyolefin elastomer is a loose talc surface coated ethylene-octene copolymer. The talc is untreated and has a nominal 1µm particle size. This product offers the exceptio.. |
|||
Density | 0.870 g/cc @Temperature 15.0 °C |
0.0314 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil Delvac 80W-140 Synthetic Gear Oil Mobil Delvac Synthetic Gear Oil 75W-90 and 80W-140 are synthetic drivetrain lubricants engineered to meet the most demanding extended drain and warranty requirements. These products are designed for.. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | ASTM D792 |
Dow Engage® ENR 7380.00 Ethylene-Butene Copolymer Description: ENR 7380.00 is a revolutionary new ethylene-butene copolymer with higher molecular weight, better toughness, and higher melt strength than other commercially available polyolefin elasto.. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | ASTM D792 |
Dow Engage® ENR 8556.00 Ethylene-Octene Copolymer Description: ENR 8556.00 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in extrusion applications such as tubing and profiles. This elastomer provides excellen.. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | ASTM D297 |
Dow Nordel® IP 4770P EPDM Hydrocarbon Rubber Description: Nordel® IP 4770P is a high molecular weight semicrystalline grade and offers fast cure rates and high states of cure with standard sulfur cure systems. It offers high green strength an.. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | ASTM D297 |
Dow Nordel® IP 4770R EPDM Hydrocarbon Rubber Description: Nordel® IP 4770R is a high molecular weight semicrystalline grade and offers fast cure rates and high states of cure with standard sulfur cure systems. It offers high green strength an.. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | |
ConocoPhillips 100 Ultra-Clean Super Hydraulic Oil Description: Conoco Ultra-Clean Super Hydraulic Oils have the same high performance characteristics of regular Super Hydraulic Oils with the added advantage of a guaranteed ISO cleanliness code of 1.. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | |
ConocoPhillips Hydroclear Diamond Class® 68 AW Turbine Oil Diamond Class AW Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited, antiwear turbine oil developed for use in geared and direct-drive gas turbines and steam turbines in severe ser.. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | |
Dow AFFINITY™ EG 8200 Polyolefin Elastomer AFFINITY® EG 8200 polyolefin elastomer is a saturated ethylene-octene copolymer for general purpose elastomeric applications that is efficiently crosslinked by peroxide, silane or irradiation. It e.. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | |
DuPont Performance Polymers Zytel® FN727 NC010A Nylon 6
(Unverified Data**) Toughened Polyamide 6Information provided by DuPont Performance Polymers |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | |
ConocoPhillips 68 Super Hydraulic Oil Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, .. |
|||
Density | 0.870 g/cc | 0.0314 lb/in³ | |
ConocoPhillips Hydroclear Diamond Class® 68 Turbine Oil Diamond Class Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited turbine oil developed for use in gas turbines and steam turbines in severe service. It is specially formulated to p.. |
|||
Density | 0.870 - 1.86 g/cc | 0.0314 - 0.0672 lb/in³ | Average value: 0.933 g/cc Grade Count:98 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi.. |