Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.600 g/cc | 0.0217 lb/in³ | true density of spheres |
Potters Industries Sphericel® 60P18 Hollow Glass Spheres Description: This microsphere is strong with a density of 0.6g/cc, and has the added advantage of a very small particle size of only 18 micron (mean). Fused glass, hollow spheres used as an additive.. |
|||
Density | 0.600 g/cc | 0.0217 lb/in³ | |
MarkeTech H-3 Honeycomb Ceramic MarkeTech International special honeycomb ceramics have a uniform lattice structure, low expansion coefficient, good thermal shock resistance, higher specific surface area, low-pressure drop, and lo.. |
|||
Density | 0.600 g/cc | 0.0217 lb/in³ | |
MarkeTech Resorcinol Formaldehyde Aerogel Monolithic resorcinol formaldehyde (RF) nanofoams are primarily used as the precursor for carbon nanofoams or when an organic, electrically insulating material is desired. The standard RF nanofoam i.. |
|||
Density | 0.600 g/cc | 0.0217 lb/in³ | |
Solvay RHODACAL® DS-10 Surfactant Identification: SODIUM DODECYLBENZENE SULFONATECAS: 69227-09-4 (TSCA) and 11067-82-6 (EINECS/ELINCS)EC Number: 234-289-1Available in: Asia Pacific, Europe, Latin America and North AmericaApplication.. |
|||
Density | 0.600 g/cc | 0.0217 lb/in³ | |
Covestro Baydur® 60 Polyurethane Rigid integral skin polyurethane foam for engineering components. The integral distribution of density gives a higher flexural modulus. If required, the property level can be improved by increasing .. |
|||
Density | 0.600 - 0.800 g/cc | 0.0217 - 0.0289 lb/in³ | ISO 845-88 |
Eurofoam Porocell POR 304 CM-OPC EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Density | 0.600 g/cc | 0.0217 lb/in³ | Typical, 3M QCM 14.24.6 |
3M HGS10000 Glass Bubbles 3M™ Glass Bubbles HGS Series are engineered hollow glass spheres for use as a density reducing agent for oil and gas drilling fluids and drilling cements. The spherical shape of 3M glass bubbles of.. |
|||
Density | 0.600 g/cc | 0.0217 lb/in³ | Typical, 3M QCM 14.24.6 |
3M HGS18000 Glass Bubbles 3M™ Glass Bubbles HGS Series are engineered hollow glass spheres for use as a density reducing agent for oil and gas drilling fluids and drilling cements. The spherical shape of 3M glass bubbles of.. |
|||
Density | 0.600 g/cc | 0.0217 lb/in³ | |
3M iM30K Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Density | 0.600 g/cc | 0.0217 lb/in³ | |
3M S60HS Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Density | 0.600 g/cc | 0.0217 lb/in³ | True Density |
3M Scotchlite™ S60/10000 Glass Bubbles High-strength polymer additives made from a water-resistant and chemically-stable soda-lime-borosilicate glass. These hollow glass microspheres can be used as a low density filler material ideal for.. |
|||
Density | 0.600 g/cc | 0.0217 lb/in³ | |
3M S60 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Density | 0.600 g/cc | 0.0217 lb/in³ | expanded |
Akzo Nobel Injection molding of 20% Wood Plastic Composite with 3.25% Expancel 092-120 |
|||
Density | 0.600 g/cc | 0.0217 lb/in³ | |
Henkel Hysol EA 9396.6MD Paste Adhesive System Cure syntactic, with excellent high temperature properties. Applications: Potting Syntactic |
|||
Density | 0.600 - 1.36 g/cc | 0.0217 - 0.0491 lb/in³ | Average value: 1.19 g/cc Grade Count:11 |
Overview of materials for ABS/PVC Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/PVC Alloy". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Density | 0.600 g/cc | 0.0217 lb/in³ | Geon® 1169; Internal Method |
PolyOne Syncure™ S1044B Polyethylene, Crosslinked (XLPE) Available as Catalyst Masterbatch component for PolyOne Syncure System.Gel values are >70, and were measured on a 90 phr S1054A / 10 phr S1044B Syncure System; and cured for 8 hours in steam. Pellet.. |