Physical Properties Metric English Comments
Density 0.481 g/cc
0.0174 lb/in³
ASTM D3574-95 Test A
Rogers Corporation Poron® 4701-41-30 Urethane Foam, Soft, Enhanced Sealability
Soft, enhanced sealability material offering greater closed-cell content for demanding vacuum sealing applications or low closure-force requirements.  Standard available thickness range from 0.031"..
Density 0.481 g/cc
0.0174 lb/in³
ASTM D3574-95 Test A
Rogers Corporation Poron® 4701-50 Supported Urethane Foam, Firm, PET Supported
Firm material used for managing high energy impact with gasketing needs.  Standard available thickness range from 0.012" to 0.500" (0.30 mm to 12.7 mm).Features and Benefits of PORON Products: Exce..
Density 0.481 g/cc
0.0174 lb/in³
ASTM D3574-95 Test A
Rogers Corporation Poron® 4701-50 Thin as Cast Urethane Foam, Firm, Thin as Cast
Firm material used for managing high energy impact with gasketing needs.  Standard available thickness range from 0.012" to 0.500" (0.30 mm to 12.7 mm).Features and Benefits of PORON Products: Exce..
Density 0.481 g/cc
0.0174 lb/in³
ASTM D3574-95 Test A
Rogers Corporation Poron® 4790-92-30012 P Urethane Foam, Extra Soft, Slow Rebound, PET Film Reinforced
Extra soft, slow rebound with a very low closure force. Available with thickness of 0.012" (0.30 mm).Features and Benefits of PORON Products: Excellent compression set resistance which enables dura..
Density >= 0.481 g/cc
>= 0.0174 lb/in³
Monmouth Rubber & Plastics Bondaflexâ„¢ B33CS Sponge Neoprene Blend
Information provided by Monmouth Rubber & Plastics Corp.
Density 0.481 - 0.641 g/cc
0.0174 - 0.0231 lb/in³
Dry
Unifrax Fiberfrax® Vari-Form™ A Casting Mix
Fiberfrax FC-25 tamping mix and Vari-Form™ castable materials provide casting mixes which can be applied in small areas such as furnace access and site doors, tube sheets, and as a refractory backu..
Density 0.481 - 0.545 g/cc
0.0174 - 0.0197 lb/in³
Engineered Syntactic Systems MZ-32 Deep Water Syntactic Foam
Syntactic foams are a unique combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having..
Density <= 0.481 g/cc
<= 0.0174 lb/in³
Engineered Syntactic Systems SF-30 Subsea Syntactic Void Filler
SF-30 is a low cost, low density syntactic formulated to serve as a void filler for shallow water subsea applications. The material is provided as a three-part kit that is mixed and poured into any ..
Density 0.481 g/cc
0.0174 lb/in³
Trelleborg AEM Eccofloat® EL-30/2000 Syntactic Foam
EL Grade epoxy syntactic foams are the material of choice for manufacturing manned and unmanned submersibles because of their density range and ability to withstand exposure to diesel fuels and hydr..
Density 0.481 g/cc
0.0174 lb/in³
ASTM D1622
Touchstone CFOAM® 30 Structural Carbon Foam
CFOAM, developed by Touchstone Research Laboratory, Ltd., is a next generation structural material which is inexpensive, lightweight, fire-resistant, impact-absorbing, and which can be thermally ins..