Polymer Property : Density = 0.400 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.400 g/cc
0.0145 lb/in³
ASTM D3574-95 Test A
Rogers Corporation Poron® 4701-30-25 Urethane Foam, Very Soft
Very soft, easily compressed for use where flexibility is a key requirement.  Standard available  thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi..
Density 0.400 g/cc
0.0145 lb/in³
ASTM D3574-95 Test A
Rogers Corporation Poron® 4701-30-25037 P Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement.  Standard available  thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi..
Density 0.400 g/cc
0.0145 lb/in³
ASTM D3574-95 Test A
Rogers Corporation Poron® 4701-30-25047 P Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement.  Standard available  thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi..
Density 0.400 g/cc
0.0145 lb/in³
±10%; ASTM D3574A
Rogers Corporation Poron® 4701-30-30 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability test MVSS 302. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -4..
Density 0.400 g/cc
0.0145 lb/in³
±10%; ASTM D3574A
Rogers Corporation Poron® 4701-40-30 Cellular Urethane Foam
Information on this material is preliminary.Standard color is black (04); others are available. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F).General Poron® information: Poron® fo..
Density 0.400 g/cc
0.0145 lb/in³
±10%; ASTM D3574A
Rogers Corporation Poron® 4701-60-30 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability test MVSS 302. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -4..
Density 0.400 g/cc
0.0145 lb/in³
Effective Density as measured by liquid displacement
Potters Industries Q-Cel® 7040S Hollow Engineered Glass Microspheres
Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths me..
Density 0.400 g/cc
0.0145 lb/in³
Pyrotek LUMIFELT AL20 High Temperature Kevlar® Felt
Lumifelt is composed of heat resistant para linked type Kevlar® fiber. Lumifelt is an ideal insulating pad for a variety of applications. It is needle punched to give it high tensile strength and..
Density 0.400 g/cc
0.0145 lb/in³
Compressed Density
Northstar Polymers MSB-M25B Microcellular Foam based on High Performance Polyester Polyurethane
This high performance polyester microcellular foam system is one of a family of polymer systems developed by Northstar Polymers for demanding work environments. Urethane foams molded with this syste..
Density 0.400 g/cc
0.0145 lb/in³
Packing Density
Northstar Polymers MSB-M25F Microcellular Foam based on High Performance Polyester Polyurethane
This high performance polyester microcellular foam system is one of a family of polymer systems developed by Northstar Polymers for demanding work environments. Urethane foams molded with this syste..
Density 0.400 - 1.24 g/cc
0.0145 - 0.0448 lb/in³
Average value: 1.07 g/cc Grade Count:70
Overview of materials for Thermoset Polyurethane, Liquid
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of..
Density 0.400 g/cc
0.0145 lb/in³
ASTM D3574-95 Test A
Rogers Corporation Poron® 4701-30-25 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film
Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement.Features and Benefits of PORON Products: Excellent compression set resistance which enab..
Density 0.400 g/cc
0.0145 lb/in³
ASTM D3574-95 Test A
Rogers Corporation Poron® 4790-92-25 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced
Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression ..
Density 0.400 g/cc
0.0145 lb/in³
ASTM D3574A
Mearthane Durethaneâ„¢ F DF-620A Closed Cell Foam Polyurethane
MDI backbone: ester.Shore 00 Hardness: 65Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient..
Density 0.400 g/cc
0.0145 lb/in³
ASTM D3574A
Mearthane Durethaneâ„¢ M DM-715A Foam Polyurethane
MDI backbone: ether.Shore 00 Hardness: 60Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Dur..
Density 0.400 g/cc
0.0145 lb/in³
Dry
Unifrax Fibermax® Duraboard® 17R Board
Duraboard® 1700 and Duraboard® 1800 are an extension to the Fibermax® product line. These board products exhibit excellent thermal stability (low shrinkage) at very high operating temperatures. ..
Density <= 0.400 g/cc
<= 0.0145 lb/in³
Engineered Syntactic Systems SF-25 Subsea Macrosphere Syntactic Void Filler
The four part SF-25 kit was developed specifically to meet the critical needs of void space filling at operating pressures to 1000 psi. This system utilizes carbon fiber reinforced epoxy macrosphere..
Density 0.400 g/cc
0.0145 lb/in³
Covestro Baydur® 40 Polyurethane
Rigid integral skin polyurethane foam for lightweight moldings. Sandwich structure gives a high stiffness-to-weight ratio.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience ..
Density 0.400 g/cc
0.0145 lb/in³
ASTM D792
Covestro Baydur® 646 Polyurethane Structural Foam RIM, Density 25 pcf, MDI-based 2-Component Liquid System
0.25 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of..
Density 0.400 g/cc
0.0145 lb/in³
Cymat A35620SC 040SS Stabilized Aluminum Foam
Description: Cymat A35620SC 040SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.4 g/cm3. The mechanical properties of SAF make it ..
Density 0.400 - 0.440 g/cc
0.0145 - 0.0159 lb/in³
ISO 845-88
Eurofoam Siliconcell 411/PLT Platinic Silicone Foam
Excellent thermal insulation and soundproofingInformation provided by Eurofoam s.r.l.
Density 0.400 g/cc
0.0145 lb/in³
ISO 845-88
Eurofoam VUL 401 Polyurethane Foam
Used for the production of springs and shock-absorbing details in the automobile industry, seals for trunks and joints for ball bearings, pressure barsInformation provided by Eurofoam s.r.l.
Density 0.400 g/cc
0.0145 lb/in³
3M Cushion-Mount™ E1215 Plus Plate Mounting Tapes with Easy Mount Adhesive
3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel..
Density 0.400 g/cc
0.0145 lb/in³
3M Cushion-Mount™ E1220 Plus Plate Mounting Tapes with Easy Mount Adhesive
3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel..
Density >= 0.400 g/cc
>= 0.0145 lb/in³
DIN 53479 A
BIW ASTM Class 2D5 Silicone Foam
Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters...
Density 0.400 g/cc
0.0145 lb/in³
ASTM D1622
Touchstone CFOAM® 25 Structural Carbon Foam
CFOAM, developed by Touchstone Research Laboratory, Ltd., is a next generation structural material which is inexpensive, lightweight, fire-resistant, impact-absorbing, and which can be thermally ins..
Density 0.400 - 0.450 g/cc
0.0145 - 0.0163 lb/in³
BASF 2,3,5-Trimethylhydroquinone
Formula: C9H12O2CAS: 700-13-0Description: TMHQ is a colorless fine crystalline powder. It is insoluble in water, soluble in methanol, ethanol, diethyl ether, and acetone.Synonyms: TMHQ, TMHApplicat..
Density 0.400 - 0.600 g/cc
0.0145 - 0.0217 lb/in³
DIN 53479 A
BIW ASTM Class 2D4 Silicone Foam
Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters...