Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0400 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.0400 g/cc
0.00145 lb/in³
ISO 845
Zotefoams ZOTEK® F 40 HT PVDF Foam
Zotek® F 40 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o..
Density 0.0400 g/cc
0.00145 lb/in³
Hexcel® HexWeb® HRH-36 - 1/8 - 2.5 Para-Aramid/Phenolic Core
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.Features: Mechanical properties equivalent to KOREX®; Low..
Density 0.0400 g/cc
0.00145 lb/in³
Hexcel® HexWeb® HRH-36/OX - 3/16 - 2.5 Para-Aramid/Phenolic Core
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.Features: Mechanical properties equivalent to KOREX®; Low..
Density 0.0400 g/cc
0.00145 lb/in³
Hexcel® HexWeb® HRH-36® Flex-Core® HRH-36 - F50 - 2.5 Aramid Honeycomb
Designation: Material-Cell Size (cells per lineal foot in W direction)-Density (lb per cubic foot)HexWeb HRH-36 Flex-Core aramid paper is reinforced with a high temperature phenolic resin. This prod..
Density 0.0400 g/cc
0.00145 lb/in³
Hexcel® HexWeb® HRP/F35 - 2.5 Nonmetallic Flex-Core Honeycomb
Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo..
Density 0.0400 g/cc
0.00145 lb/in³
Hexcel® HexWeb® HRH-10/F35 - 2.5 Nonmetallic Flex-Core Honeycomb
Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo..
Density 0.0400 - 0.0600 g/cc
0.00145 - 0.00217 lb/in³
ISO 845-88
Eurofoam Evacell EVA 50/S EVA + NR Foam
Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di..
Density 0.0400 - 0.0500 g/cc
0.00145 - 0.00181 lb/in³
ISO 845-88
Eurofoam Polycell PLZ 45 Polyethylene Foam
Information provided by Eurofoam s.r.l.
Density 0.0400 g/cc
0.00145 lb/in³
DIN 53420
Dow STRANDFOAM™ EA 1000 Polypropylene Foam
STRANDFOAM™ EA 1000 Energy Absorbing polypropylene foam is a strong, low-density, closed-cell foam. It is suited as a component material in products requiring a shock and energy absorbing or vibra..
Density 0.0400 g/cc
0.00145 lb/in³
ISO 845
BASF Neopolen® P 8015 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8015 is expanded Polypropylene supplied in the form of beads. The cells are largely closed. Physical properties of moldings made from Neopolen® P 8015Note: In order to mea..
Density 0.0400 g/cc
0.00145 lb/in³
ISO 845
BASF Neopolen® P 8225 K 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to..
Density 0.0400 g/cc
0.00145 lb/in³
ISO 845
BASF Neopolen® P 9035 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9035 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9035.Note: In order to mea..
Density 0.0400 g/cc
0.00145 lb/in³
ISO 845
BASF Neopolen® P 9225 K 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to..
Density 0.0400 g/cc
0.00145 lb/in³
ISO 845
BASF Neopolen® P 9230 D 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to..
Density 0.0400 g/cc
0.00145 lb/in³
ISO 845
BASF Neopolen® P 9230 K 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to..
Density 0.0400 g/cc
0.00145 lb/in³
ISO 845
BASF Neopolen® P 9235 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea..
Density 0.0400 g/cc
0.00145 lb/in³
ISO 845
BASF Neopolen® P 9335 MG 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order ..
Density 0.0400 g/cc
0.00145 lb/in³
ISO 845
BASF Neopolen® P 9435 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea..
Density 0.0400 g/cc
0.00145 lb/in³
ISO 845
BASF Neopolen® P 9230 A 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to..
Density 0.0400 g/cc
0.00145 lb/in³
ISO 845
BASF Neopolen® P 8220 K 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8220 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8220 K.Note: In order to..
Density 0.0400 - 0.0800 g/cc
0.00145 - 0.00289 lb/in³
molding density range
IRPC Polimaxx Pentfoam 522F Expandable Polystyrene
GENERAL: PENTFOAM "522F" IS A REGULAR GRADE (STANDARD GRADE) EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT. THIS GRADE IS DEVELOPED TO MEET THE DEMAND FOR FAST MOLDING CYCLES IN V..
Density 0.0400 - 0.0800 g/cc
0.00145 - 0.00289 lb/in³
molding density range
IRPC Polimaxx Pentfoam 526W Expandable Polystyrene
GENERAL: PENTFOAM "526W" IS A REGULAR GRADE (STANDARD GRADE) EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT.APPLICATIONS: PENTFOAM "526W" IS PARTICULARLY WELL SUITED FOR THE MANUFA..
Density 0.0400 g/cc
0.00145 lb/in³
average; ISO 845
3A Composites Core Materials AIREX® C70.40 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible ..
Copyright © lookpolymers.com All Rights Reserved