Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | >= 0.0120 g/cc | >= 0.000434 lb/in³ | Minimum apparent density on a continuous pre-expander after two expansions |
Polimeri Europa Extir® CM Galileo Europa 5 AE Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Density | 0.0120 - 0.0250 g/cc | 0.000434 - 0.000903 lb/in³ | Density range normally used |
Polimeri Europa Extir® CM Galileo Europa 5 AE Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Density | 0.0120 - 0.0250 g/cc | 0.000434 - 0.000903 lb/in³ | Density range normally used |
Polimeri Europa Extir® CM Galileo Europa 5 Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Density | >= 0.0120 g/cc | >= 0.000434 lb/in³ | Double Pass Continuous Expansion |
NOVA Chemicals EPS 33MA Modified Expandable Polystyrene Applications: Insulation, bean bags, SIP's, ICF'sInformation provided by NOVA Chemicals. |
|||
Density | >= 0.0120 g/cc | >= 0.000434 lb/in³ | Double Pass Continuous Expansion |
NOVA Chemicals EPS M77A Expandable Polystyrene Resin Applications Insulation, Bean bag, SIP'sInformation provided by NOVA Chemicals |
|||
Density | >= 0.0120 g/cc | >= 0.000434 lb/in³ | Double Pass Continuous Expansion |
NOVA Chemicals EPS M77B Expandable Polystyrene Resin Applications Insulation, SIP's, Fabricated PackagingInformation provided by NOVA Chemicals |
|||
Density | >= 0.0120 g/cc | >= 0.000434 lb/in³ | Double Pass Continuous Expansion |
NOVA Chemicals EPS M77B Modified Expandable Polystyrene Applications: Insulation, SIP's, ICF's, fabricated packagingInformation provided by NOVA Chemicals. |
|||
Density | >= 0.0120 g/cc | >= 0.000434 lb/in³ | Minimum apparent density on a continuous pre-expander after two expansions |
Polimeri Europa Extir® CM Galileo Io 5 AE Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Density | 0.0120 - 0.0250 g/cc | 0.000434 - 0.000903 lb/in³ | Density range normally used |
Polimeri Europa Extir® CM Galileo Io 5 AE Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Density | >= 0.0120 g/cc | >= 0.000434 lb/in³ | Minimum apparent density on a continuous pre-expander after two expansions |
Polimeri Europa Extir® CM Galileo Io 5 Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Density | 0.0120 - 0.0250 g/cc | 0.000434 - 0.000903 lb/in³ | Density range normally used |
Polimeri Europa Extir® CM Galileo Io 5 Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Density | 0.0120 - 0.0250 g/cc | 0.000434 - 0.000903 lb/in³ | Density range normally used |
Polimeri Europa Extir® CM Giotto 5 Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Density | 0.0120 - 0.0300 g/cc | 0.000434 - 0.00108 lb/in³ | |
Polimeri Europa Extir® D 5000 AE Expandable Polystyrene
(discontinued **) Extir D 5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Ext.. |
|||
Density | 0.0120 - 0.0300 g/cc | 0.000434 - 0.00108 lb/in³ | Density range normally used |
Polimeri Europa Extir® PD D 5000 AE Expandable Polystyrene, Fast Molding Flame Retardant
(discontinued **)< Particle size range is 0.9 - 1.6 mm. Minimum apparent density after two expansions is 11 g/l. Minimum apparent density on a discontinuous pre-expander is 14 g/l. Minimum apparent density on a cont.. |
|||
Density | 0.0120 - 0.0200 g/cc | 0.000434 - 0.000723 lb/in³ | Density range normally used |
Polimeri Europa Extir® A 2000/1 Expandable Polystyrene, Special Purpose
(discontinued **) Particle size range is 0.4 - 0.75 mm. Minimum apparent density after two expansions is 12 g/l. Minimum apparent density on a discontinuous pre-expander is 12 g/l. Minimum apparent density on a con.. |
|||
Density | >= 0.0120 g/cc | >= 0.000434 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
NOVA Chemicals Styrocell® B933A Expandable Polystyrene
(discontinued **) This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used as expansion agent, typically used as pre-expanded beads in the .. |
|||
Density | >= 0.0120 g/cc | >= 0.000434 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
Ineos Nova T163B Expandable Polystyrene A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for very low density foam.Applications: This grade is used mainl.. |
|||
Density | >= 0.0120 g/cc | >= 0.000434 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
Ineos Nova T243C Expandable Polystyrene A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for low and standard density foam.Applications: This grade is us.. |
|||
Density | >= 0.0120 g/cc | >= 0.000434 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
Ineos Nova T733B Expandable Polystyrene A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used after expansion for cellular bricks.Applications: This grade is.. |
|||
Density | 0.0120 - 0.0130 g/cc | 0.000434 - 0.000470 lb/in³ | |
IRPC Polimaxx Pentfoam 155E Expandable Polystyrene General: Pentfoam 155E is a self extinguising grad expandable polystyrene containing pentate as blowing agentApplications: Pentfoam 155E is particularly well suited for the manufacture of low densit.. |
|||
Density | 0.0120 - 0.0200 g/cc | 0.000434 - 0.000723 lb/in³ | molding density range |
IRPC Polimaxx Pentfoam 155E Expandable Polystyrene General: Pentfoam 155E is a self extinguising grad expandable polystyrene containing pentate as blowing agentApplications: Pentfoam 155E is particularly well suited for the manufacture of low densit.. |
|||
Density | 0.0120 - 0.0130 g/cc | 0.000434 - 0.000470 lb/in³ | |
IRPC Polimaxx Pentfoam 193L Expandable Polystyrene General: Pentfoam 139L is a regular grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast molding cycles in vacuum machine.Application.. |
|||
Density | 0.0120 - 0.0200 g/cc | 0.000434 - 0.000723 lb/in³ | molding density range |
IRPC Polimaxx Pentfoam 193L Expandable Polystyrene General: Pentfoam 139L is a regular grade expandable polystyrene containing pentane as blowing agent. This grade is developed to meet the demand for fast molding cycles in vacuum machine.Application.. |
|||
Density | 0.0120 - 0.0200 g/cc | 0.000434 - 0.000723 lb/in³ | molding density range |
IRPC Polimaxx Pentfoam 241F Expandable Polystyrene General: Pentfoam 241F is a regular grade expandable polystyrene containing pentane as blowing agentApplications: Pentfoam 241F is particularly well suited for the manufacture of eps insulation boar.. |
|||
Density | 0.0120 - 0.020 g/cc | 0.000434 - 0.00072 lb/in³ | expanded |
Jackon JACKOCELL® R211 Expanded Polystyrene Construction and Block Molding High quality processingHigh strengthLow wasteFast moulding cycles |
|||
Density | 0.0120 - 0.0200 g/cc | 0.000434 - 0.000723 lb/in³ | expanded |
Jackon JACKOCELL® R212 Expanded Polystyrene Construction and Block Molding High quality processingHigh strengthLow wasteFast moulding cycles |
|||
Density | 0.0120 g/cc | 0.000434 lb/in³ | 95 second cycle time |
Jackon JACKOCELL® S214 Expanded Polystyrene Construction and Block Molding Pre-ExpansionThe unique design of polystyrene chains and additive chemistry in Jackocell® S214 gives pre-expanded beads high dimensional stability even at low densities, which typically reduces a.. |
|||
Density | <= 0.0120 g/cc | <= 0.000434 lb/in³ | TMA |
Akzo Nobel Expancel® 950 DU 80 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | 0.0120 - 0.0300 g/cc | 0.000434 - 0.00108 lb/in³ | Density range normally used |
Polimeri Europa Extir® D 5000 AE Expandable Polystyrene - Flame Retardant Product Description:Extir D 5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent.Extir does not conta.. |
|||
Density | <= 0.0120 g/cc | <= 0.000434 lb/in³ | TMA |
Akzo Nobel Expancel® 950 DU 120 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |