Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zeon Chemicals Zetpol® 1010 Hydrogenated Nitrile Elastomomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name Zetpol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Zetpol® 1010 Hydrogenated Nitrile Elastomomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Zeptol 1010 is a highly saturated copolymer of butadiene and acrylonitrile with high tensile strength, good heat resistance, good chemical reistance to aggressive fluids, and an excellent balance of properties over a wide variation of temperatures.For fuel-resistant hoses, diaphragms, and seals. Automotive and industrial refrigerant applications, FDA approved.
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
Iodine Absorption Number 7.0 - 13
7.0 - 13
mg/100mg; ZCI-T-004
Mooney Viscosity 78 - 92

@Temperature 100 °C
78 - 92

@Temperature 212 °F
(1+4); ZCI-T-003
Ash <= 0.50 %
<= 0.50 %
ZCI-T-005
Mechanical Properties Metric English Comments
Hardness, Shore A >= 67
>= 67
ZCI-T-009
Tensile Strength at Break >= 19.50 MPa
>= 2828 psi
ZCI-T-008
Elongation at Break >= 300 %
>= 300 %
ZCI-T-008
300% Modulus >= 0.009797 GPa
>= 1.421 ksi
ZCI-T-008
Descriptive Properties Value Comments
% HYD 96
Bound ACN (%, acrylonitrile) 42.9-45.5
Heat Loss (%) Max 0.5