Zeon Chemicals Nipol® 33-5HM Nitrile Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name Nipol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Nipol® 33-5HM Nitrile Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Low mold fouling, high-modulus, 55 Mooney nitrile rubber, recommended for high temperature injection molding.Low mold fouling, high-modulus, 55 Mooney nitrile rubber. Recommended for high temperature injection molding.
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
Mooney Viscosity 47 - 57

@Temperature 100 °C
47 - 57

@Temperature 212 °F
(1+4)
Ash <= 0.75 %
<= 0.75 %
T-4210
Descriptive Properties Value Comments
AO Type NS
Bound ACN (%, acrylonitrile) 32-34
Heat Loss (%) Max 0.5
Hot/Cold C