| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
| Water Absorption | 0.010 % @Temperature 23.0 °C |
0.010 % @Temperature 73.4 °F |
RMC 93%; DIN EN ISO 62 |
| Moisture Absorption at Equilibrium | 0.050 % | 0.050 % | DIN EN ISO 62 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | >= 100 | >= 100 | DIN 53505 |
| Hardness, Shore D | 81 | 81 | DIN 53505 |
| Ball Indentation Hardness | 107 MPa | 15500 psi | DIN 2039 |
| Tensile Strength at Break | 50.0 MPa | 7250 psi | DIN EN ISO 527 |
| Tensile Strength | 50.0 MPa | 7250 psi | DIN EN ISO 527 |
| Tensile Stress | 14.0 MPa @Strain 1.00 %, Time 3.60e+6 sec |
2030 psi @Strain 1.00 %, Time 1000 hour |
DIN 53444 |
| Tensile Strength, Yield | 38.0 MPa | 5510 psi | Elastic Limit |
| Elongation at Break | 19.9 % | 19.9 % | |
| 19.9 % | 19.9 % | DIN EN ISO 527 | |
| Elongation at Yield | 3.4 % | 3.4 % | Elastic Yield Point |
| 5.6 % | 5.6 % | Flexural; DIN EN ISO 178 | |
| 19.9 % | 19.9 % | Elongation at Maximum Force; DIN EN ISO 527 | |
| Tensile Modulus | 1.50 GPa | 218 ksi | DIN EN ISO 527 |
| Flexural Strength | 63.0 MPa | 9140 psi | Outer Fiber Stress at 3.5% Outer Fiber Strain; DIN EN ISO 178 |
| 70.0 MPa | 10200 psi | DIN EN ISO 178 | |
| Flexural Modulus | 2.32 GPa | 336 ksi | DIN EN ISO 178 |
| Compressive Strength | 50.4 MPa | 7310 psi | Elastic Limit |
| 19.0 MPa @Time 3.60e+7 sec |
2760 psi @Time 10000 hour |
||
| 43.0 MPa @Time 360000 sec |
6240 psi @Time 100 hour |
||
| 54.0 MPa @Time 36.0 sec |
7830 psi @Time 0.0100 hour |
||
| 40.5 MPa @Strain 3.50 % |
5870 psi @Strain 3.50 % |
DIN EN ISO 604 | |
| Compressive Modulus | 1.748 GPa | 253.5 ksi | DIN EN ISO 604 |
| Fatigue Strength | 6.00 MPa @# of Cycles 1.00e+6 |
870 psi @# of Cycles 1.00e+6 |
1 Hz |
| K Factor (ISO) | 0.30 µm/km @Temperature 20.0 °C |
0.30 µm/km @Temperature 68.0 °F |
|
| 1.0 µm/km @Temperature 100 °C |
1.0 µm/km @Temperature 212 °F |
||
| Charpy Impact Unnotched | NB | NB | EN ISO 179/1eU |
| Charpy Impact, Notched | 2.35 J/cm² | 11.2 ft-lb/in² | EN ISO 179/1eA |
| Coefficient of Friction, Dynamic | 0.080 @Temperature 100 °C |
0.080 @Temperature 212 °F |
Dry Operation |
| 0.13 @Temperature 20.0 °C |
0.13 @Temperature 68.0 °F |
Dry Operation | |
| Coefficient of Friction, Static | 0.21 @Temperature 20.0 °C |
0.21 @Temperature 68.0 °F |
Dry Operation |
| Tensile Creep Modulus, 1000 hours | 1300 MPa | 189000 psi | At 1% Deformation; DIN 53444 |
| Limiting Pressure Velocity | 0.150 MPa-m/sec | 4280 psi-ft/min | v = 100m/min |
| 0.16667 MPa-m/sec | 4758.4 psi-ft/min | v = 200m/min | |
| 0.35583 MPa-m/sec | 10159 psi-ft/min | v = 1m/min | |
| 0.96666 MPa-m/sec | 27598 psi-ft/min | v = 10m/min | |
| Compression Set | 4.5 % | 4.5 % | Elastic Compression Limit |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 60.0 µm/m-°C @Temperature <=100 °C |
33.3 µin/in-°F @Temperature <=212 °F |
ISO E 830 |
| 67.0 µm/m-°C @Temperature <=150 °C |
37.2 µin/in-°F @Temperature <=302 °F |
ISO E 831 | |
| Specific Heat Capacity | 1.81 J/g-°C | 0.433 BTU/lb-°F | DSC |
| Melting Point | 320 °C | 608 °F | DSC |
| Maximum Service Temperature, Air | 70.0 °C | 158 °F | Pressed Bushings |
| 160 °C | 320 °F | Short Term (3h) | |
| 170 °C | 338 °F | Continuous | |
| Deflection Temperature at 1.8 MPa (264 psi) | 117 °C | 243 °F | DIN EN ISO 75 |
| Glass Transition Temp, Tg | 90.0 °C | 194 °F | DSC |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | IEC 93 |
| Surface Resistance | 6.50e+12 ohm | 6.50e+12 ohm | IEC 93 |
| Dielectric Constant | 4.1 @Frequency 110 Hz |
4.1 @Frequency 110 Hz |
IEC 250 |
| Dielectric Strength | 21.5 kV/mm | 546 kV/in | IEC 243 |
| Dissipation Factor | 0.030 | 0.030 | IEC 112 |
| 0.11 @Frequency 1.00 Hz |
0.11 @Frequency 1.00 Hz |
||
| Comparative Tracking Index | 130 V | 130 V | IEC 112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Alignment Adjustment | 5 | Nominal Scale: 1, low; 10, high |
| Chemical Sterilization | 10 | Nominal Scale: 1, low; 10, high |
| Color | Beige | |
| Creep Resistance | 2 | Nominal Scale: 1, low; 10, high |
| Dimensional Stability with Thermal Expansion | 5 | Nominal Scale: 1, low; 10, high |
| FDA Compliant | Applicable | |
| Free from Silicon | Applicable | |
| Gamma-rays Radiation Sterilization | 4 | Nominal Scale: 1, low; 10, high |
| Injection Molded Parts | Applicable | |
| Machined Parts | Applicable | |
| Moist Heat Sterilization | 7 | Nominal Scale: 1, low; 10, high |
| Plastic Granules | Applicable | |
| Resistance Against dust, Dirt, Abrasive Substances | 7 | Nominal Scale: 1, low; 10, high |
| Resistance Against Hot Water | 140 | |
| Resistance to Chemicals | 5 | Nominal Scale: 1, low; 10, high |
| Resistant Against Disinfectant | Applicable | |
| Rods up to Øe (de) | Applicable | |
| Sheets up to Maximum Thickness | Applicable | |
| Sliding Velocity | 50 | |
| Suitable for Outdoor Use | 7 | Nominal Scale: 1, low; 10, high |
| Suitable for Vacuum | Applicable | |
| Tubes (hollow rods) up to Øe (de) | Applicable | |
| UV Rays Resistance | 8 | Nominal Scale: 1, low; 10, high |
| UV-Sterilization | 7 | Nominal Scale: 1, low; 10, high |