Material Notes:
WESTLAKE low-density polyethylene EC474 is a general-purpose formulation used for extrusion coating and laminating. It can be drawn down to low coating weights, is processable at high speeds, has good moisture barrier, and is heat-sealable at low temperatures.Application/UsesMedium and lightweight coatings and laminationsSubstrate coatings to provide heat sealabilityHot melt laminating adhesiveGeneral purpose coatingsFDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ASTM D1505
Melt Flow 8.0 g/10 min
8.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 9.65 MPa
1400 psi
ASTM D638
Elongation at Break 400 %
400 %
ASTM D638
Tensile Modulus 0.138 GPa
20.0 ksi
ASTM D1709
Processing Properties Metric English Comments
Melt Temperature 302 - 329 °C
575 - 625 °F
Descriptive Properties Value Comments
Process Coating
Region US & Canada