Victrex® Vicote® F813 Black Polyetheretherketone (PEEK) Liquid Dispersion

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer Victrex
Trade Name Vicote®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Victrex® Vicote® F813 Black Polyetheretherketone (PEEK) Liquid Dispersion.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
VICOTE® is the brand name for the Victrex range of coatings. The VICOTE Coatings are available through Victrex plc or its preferred coater network. The VICOTE F813Blk grade has been specifically formulated to provide a coating that gives high wear and abrasion resistance combined with excellent release properties that are retained as the coating wears. These properties are retained at high temperatures where other release coatings would potentially fail. VICOTE dispersions coatings have a low level of extractables.All information provided by Victrex.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ISO 2811
Solids Content 26 %
26 %
Theory Volume
36.9 %
36.9 %
weight; Internal Test
pH 10
10
Viscosity Measurement 12

@Temperature 25.0 °C
12

@Temperature 77.0 °F
BSEN ISO 2431
Mechanical Properties Metric English Comments
Impact 1.0
1.0
1m, 2kg, Indent 5mm; ISO 6272
Coefficient of Friction 0.021
0.021
µm @ 10 min., Using 250N Load; ASTM G 133
Thermal Properties Metric English Comments
Melting Point 372 °C
702 °F
DSC
Softening Point 260 °C
500 °F
Processing Properties Metric English Comments
Drying Temperature 120 °C
248 °F
overnight before use
150 °C

@Time 10800 sec
302 °F

@Time 3.00 hour
Descriptive Properties Value Comments
Bend (mm) Pass at 3.2
ISO 6860
Color Black
Konig Hardness (seconds) 105
ISO 1522