Universal Wire Works 6130 (AMS 6462) Low Alloy Steel Welding Wire

Category Metal , Ferrous Metal , Alloy Steel , Low Alloy Steel
Manufacturer Universal Wire Works
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works 6130 (AMS 6462) Low Alloy Steel Welding Wire.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Alloy 6130 is primarily used with the gas tungsten arc, gas metal arc and submerged arc welding processes. This low-alloy filler metal is designed to weld low-alloy steels capable of heat treatment of 150,000 psi tensile strength.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Component Elements Properties Metric English Comments
Carbon, C 0.30 %
0.30 %
Chromium, Cr 1.0 %
1.0 %
Copper, Cu <= 0.35 %
<= 0.35 %
Iron, Fe >= 96.7 %
>= 96.7 %
As Remainder
Manganese, Mn 0.80 %
0.80 %
Molybdenum, Mo <= 0.060 %
<= 0.060 %
Nickel, Ni <= 0.25 %
<= 0.25 %
Phosphorous, P <= 0.025 %
<= 0.025 %
Silicon, Si 0.25 %
0.25 %
Sulfur, S <= 0.025 %
<= 0.025 %
Vanadium, V 0.20 %
0.20 %