Universal Wire Works 17-22ASVM (AMS 6458) Low Alloy Steel Welding Wire

Category Metal , Ferrous Metal , Alloy Steel , Low Alloy Steel
Manufacturer Universal Wire Works
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works 17-22ASVM (AMS 6458) Low Alloy Steel Welding Wire.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Alloy 17-22ASVM is a controlled chemistry vacuum melted filler metal of premium quality. This alloy is primarily used with the gas tungsten arc and gas metal arc processes for low alloy steels of similar composition where the weld metal is required to have strength comparable to that of the parent metal.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Component Elements Properties Metric English Comments
Carbon, C 0.30 %
0.30 %
Chromium, Cr 1.25 %
1.25 %
Copper, Cu <= 0.35 %
<= 0.35 %
Hydrogen, H <= 0.0025 %
<= 0.0025 %
Iron, Fe >= 95.8 %
>= 95.8 %
As Remainder
Manganese, Mn 0.55 %
0.55 %
Molybdenum, Mo 0.50 %
0.50 %
Nickel, Ni <= 0.25 %
<= 0.25 %
Nitrogen, N <= 0.0050 %
<= 0.0050 %
Oxygen, O <= 0.0025 %
<= 0.0025 %
Phosphorous, P <= 0.0080 %
<= 0.0080 %
Silicon, Si 0.65 %
0.65 %
Sulfur, S <= 0.0080 %
<= 0.0080 %
Vanadium, V 0.30 %
0.30 %