Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Tra-Con Tra-Coat CF103B UV Curable Rigid Coating

Category Other Engineering Material , Ceramic/Metallic Coating , Polymer , Adhesive , Thermoset
Manufacturer Tra-Con, Inc.
Trade Name Tra-Coat
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Coat CF103B UV Curable Rigid Coating.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
TRA-COAT CF103B is a high-gloss, UV curable polymer coating. It provides a wear layer with outstanding gloss retention, moisture resistance, stain resistance, and abrasion resistance. It can be used as a low maintenance finish for metals, plastics, and ceramics. It’s proven uses include ski and snowboard coating and decorative lamination. TRA-COAT CF103B will cure at 30 feet per minute at 300 watt/inch intensity. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Viscosity 130 cP

@Temperature 60.0 °C
130 cP

@Temperature 140 °F
Adhesive (cp #40, 20 rpm)
215 cP

@Temperature 50.0 °C
215 cP

@Temperature 122 °F
Adhesive (cp #40, 20 rpm)
350 cP

@Temperature 40.0 °C
350 cP

@Temperature 104 °F
Adhesive (cp #40, 20 rpm)
670 cP

@Temperature 30.0 °C
670 cP

@Temperature 86.0 °F
Adhesive (cp #40, 20 rpm)
1100 cP

@Temperature 25.0 °C
1100 cP

@Temperature 77.0 °F
Adhesive (cp #40, 20 rpm)
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
Hardness, Shore D 60
60
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 22.0 °C
71.6 °F
Ultimate Tg
Descriptive Properties Value Comments
Color Clear
Mixed/Cured
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved