Tra-Con Tra-Bond 226U01 High Temperature Controlled Flow Adhesive

Category Polymer , Adhesive , Thermoset
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond 226U01 High Temperature Controlled Flow Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
TRA-BOND 226U01 is a one-part, controlled flow adhesive with high temperature resistance.Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
Cured
Viscosity 250000 cP
250000 cP
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore D 90
90
24 hrs @ 75°C
Adhesive Bond Strength 26.9 MPa
3900 psi
Lap shear, alum to alum, 1 hr @ 150°C
Thermal Properties Metric English Comments
CTE, linear 45.0 µm/m-°C

@Temperature 20.0 °C
25.0 µin/in-°F

@Temperature 68.0 °F
Alpha 1
160 µm/m-°C

@Temperature 20.0 °C
88.9 µin/in-°F

@Temperature 68.0 °F
Alpha 2
Glass Transition Temp, Tg 135 °C
275 °F
Ultimate Tg
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 150 °C
1.00 hour

@Temperature 302 °F
Descriptive Properties Value Comments
Color Blue