Material Notes:
Notes: The Specialty Compounding Division offers a proprietary line of cap-liner compounds designed for carbonated soft drinks. These are proven products that have been used commercially for several years. These compounds are available pre-colored or natural, and can be tailored to specific needs. Forms: PelletsInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Melt Flow 12.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
12.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 88
88
15 seconds; ASTM D2240
Tensile Strength at Break 7.58 MPa
1100 psi
ASTM D638
Elongation at Break 470 %
470 %
ASTM D638
Users viewing this material also viewed the following: