| Category | Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber |
| Manufacturer | Teknor Apex Company |
| Trade Name | TEKRON® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Teknor Apex TEKRON® 4300-D88F Thermoplastic Elastomer.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.900 g/cc | 0.900 g/cc | +/- 0.02; ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.0090 cm/cm | 0.0090 in/in | at 80°C for 30 min. |
| 0.0090 cm/cm | 0.0090 in/in | ||
| 0.012 cm/cm | 0.012 in/in | at 93°C for 30 min. | |
| Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | at 80°C for 30 min. |
| 0.010 cm/cm | 0.010 in/in | ||
| 0.013 cm/cm | 0.013 in/in | at 93°C for 30 min. | |
| Melt Flow | 12 g/10 min @Load 2.16 kg, Temperature 230 °C |
12 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 38 | 38 | 10 second delay. +/- 3; ASTM D2240 |
| Tensile Strength, Yield | 9.86 MPa | 1430 psi | ASTM D412 |
| Elongation at Break | 415 % | 415 % | ASTM D412 |
| Flexural Modulus | 0.1500 GPa | 21.75 ksi | ASTM D790 |
| 0.0620 GPa @Temperature 70.0 °C |
8.99 ksi @Temperature 158 °F |
ASTM D790 | |
| 2.079 GPa @Temperature -30.0 °C |
301.6 ksi @Temperature -22.0 °F |
ASTM D790 | |
| Impact Test | 18.4 J @Temperature 23.0 °C |
13.6 ft-lb @Temperature 73.4 °F |
Multi-axial, at max. load |
| 22.4 J @Temperature -40.0 °C |
16.5 ft-lb @Temperature -40.0 °F |
Multiaxial, Peak Lead | |
| Tear Strength | 63.1 kN/m | 360 pli | Die C; ASTM D1004 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
| Flame Spread | 25.4 mm/min | 1.00 in/min | Pass: Burn Rate- Max 100; FMVSS 302 |