Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex Sinvicomp SIM 5520 Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade
Manufacturer Teknor Apex Company
Trade Name Sinvicomp
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Sinvicomp SIM 5520 Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability: Asia Pacific Features: High Strength Uses: Electrical/Electronic Applications < Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
ASTM D2240
Tensile Strength, Yield 17.0 MPa
2470 psi
9.8 in/min; ASTM D638
Elongation at Break 300 %
300 %
590 in/min; ASTM D638