Teknor Apex HFFR 2006 Polyolefin, Halogen Free

Category Polymer , Thermoplastic , Polyolefin , Polyolefin, Wire/Cable Grade
Manufacturer Teknor Apex Company
Trade Name HFFR
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex HFFR 2006 Polyolefin, Halogen Free.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Notes: RoHS Compliant Features: Flame Retardant; Halogen Free Uses: Communication Wire Jacketing; Electronic Cable Jacketing; Security Cable Jacketing Agency Ratings: IEC Unspecified Rating; ICEA Unspecified Rating Processing Method: Extrusion Forms: Pellets Additional Information: Ultimate Elongation Retained, UL 1581, Oven Aged, 7 days, 100°C: 75% Tensile Strength Retained, UL 1581, Oven Aged, 7 days, 100°C: 101% Acid Gas, MIL-C-24643: < 5.0 mg Acidity of Gases, IEC-754-2: < 6.0 pH Conductivity: < 2.0 µS/cm Smoke Index, NES-711: < 7.5 Toxicity Index, NES-713: 0.025 Cone Calorimeter at 50 kW/m2, Peak Heat Release Rate: 430 kW/m2 Cone Calorimeter at 50 kW/m2, Total Heat Released: 140 MJ/m2 Cone Calorimeter at 50 kW/m2, Peak Smoke: 1.9 1/m Cone Calorimeter at 50 kW/m2, Time to Sustained Ignition: 91 secInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
Melt Flow 7.60 g/10 min

@Load 10.0 kg,
Temperature 190 °C
7.60 g/10 min

@Load 22.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 41
41
10 seconds; ASTM D2240
Tensile Strength at Break 8.27 MPa
1200 psi
ASTM D638
Elongation at Break 390 %
390 %
ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -28.0 °C
-18.4 °F
ASTM D746
Oxygen Index 35 %
35 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 1.10e+13 ohm-cm
1.10e+13 ohm-cm
ASTM D257
Dielectric Constant 3.68

@Frequency 1000 Hz
3.68

@Frequency 1000 Hz
ASTM D150
Dissipation Factor 0.0067

@Frequency 1000 Hz
0.0067

@Frequency 1000 Hz
ASTM D150
Descriptive Properties Value Comments
Appearance Opaque