Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex Fireguard® 910L16-C1A-NL1 Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name Fireguard®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Fireguard® 910L16-C1A-NL1 Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Notes: RoHS Compliant Features: Flame Retardant; Low Smoke Emission Uses: Plenum Cable Jacketing Wire Types: CL2P; CL3P; CMP; FPLP; MPP; OFNP Agency Ratings: NEC Article 725; NEC Article 760; NEC Article 770; NEC Article 800; UL 13; UL 1424; UL 1651; UL 444; UL QMTT2 .E200337 Processing Method: Extrusion Forms: Pellets Additional Notes: Dynamic Heat Stability at 205°C, 100 rpm, 72 gr. #5 Bowl (Minutes to Decomposition): 34 Kayness ACR at 370°F, 1000 sec-1: 315 Pa-s Kayness ACR at 370°F, 100 sec-1: 1243 Pa-sPeak Heat Release Rate: 120 kW/m2 Average Heat Release Rate: 69 kW/m2 Total Heat Released: 65 MJ/m2 Average Heat of Combustion: 10.3 MJ/kg Average Specification Extinction Area: 316 m2/kg Peak Smoke: 1.91 1/mInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.62 g/cc
1.62 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore C 80
80
10 seconds; ASTM D2240
89
89
ASTM D2240
Tensile Strength at Break 14.5 MPa
2100 psi
ASTM D638
Elongation at Break 270 %
270 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 60.0 °C
140 °F
Continuous Use; ASTM D794
Brittleness Temperature -25.0 °C
-13.0 °F
ASTM D746
Oxygen Index 51 %
51 %
ASTM D2863
Electrical Properties Metric English Comments
Dielectric Constant 3.58

@Frequency 1.00e+6 Hz
3.58

@Frequency 1.00e+6 Hz
ASTM D150
4.56

@Frequency 1000 Hz
4.56

@Frequency 1000 Hz
ASTM D150
Dissipation Factor 0.038

@Frequency 1.00e+6 Hz
0.038

@Frequency 1.00e+6 Hz
ASTM D150
0.065

@Frequency 1000 Hz
0.065

@Frequency 1000 Hz
ASTM D150
Processing Properties Metric English Comments
Melt Temperature 193 °C
380 °F
Descriptive Properties Value Comments
Appearance Opaque
Users viewing this material also viewed the following: