Teknor Apex APEX® CX 2001-84 Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® CX 2001-84 Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Notes: RoHS Compliant Features: Flame Retardant Uses: Cable Jacketing; Coaxial Cable Jacketing Agency Ratings: UL 444; UL 62Processing Method: Extrusion Forms: Pellets Additional Information: Temperature Rating: 75°C UL Sunlight Resistance Recognition: NoInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.42 g/cc
1.42 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 84
84
15 seconds; ASTM D2240
Tensile Strength at Break 15.2 MPa
2200 psi
ASTM D638
Elongation at Break 310 %
310 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 80.0 °C
176 °F
Continuous Use; ASTM D794
Brittleness Temperature -22.0 °C
-7.60 °F
ASTM D746
Oxygen Index 29 %
29 %
ASTM D2863
Descriptive Properties Value Comments
Appearance Opaque