Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Taiwan Sheen Soon Sheenthane® A8557E2 Thermoplastic Polyurethane Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer Taiwan Sheen Soon Co. Ltd.
Trade Name Sheenthane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Taiwan Sheen Soon Sheenthane® A8557E2 Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Thermoplastic polyurethane elastomer for extrusionPolyether gradeInformation provided by Taiwan Sheen Soon Co., LTD.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 83 - 87
83 - 87
Tensile Strength 27.5 MPa
3980 psi
Elongation at Break 700 %
700 %
100% Modulus 0.00441 GPa
0.639 ksi
300% Modulus 0.00735 GPa
1.07 ksi
Processing Properties Metric English Comments
Processing Temperature 175 - 205 °C
347 - 401 °F