Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Taiwan PU Corporation TPU-BTB85 Breathable Grade, Blow Molding Polyether Base TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Taiwan PU Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Taiwan PU Corporation TPU-BTB85 Breathable Grade, Blow Molding Polyether Base TPU.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Thermoplastic Polyurethane (TPU), Breathable Grade, Polyether Base, Blow MoldingInformation provided by Taiwan PU Corporation.
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
Tensile Strength at Break 27.46 MPa
3983 psi
Elongation at Break 750 %
750 %
100% Modulus 0.00440 GPa
0.638 ksi
300% Modulus 0.00690 GPa
1.00 ksi
Resilience 45
45
%, Impact Resilience
Taber Abrasion, mg/1000 Cycles 15
15
Processing Properties Metric English Comments
Feed Temperature 175 °C
347 °F
Middle Barrel Temperature 180 °C
356 °F
Compress zone
Front Barrel Temperature 185 °C
365 °F
Metering zone
Adapter Temperature 190 °C
374 °F
Die Temperature 190 °C
374 °F
Users viewing this material also viewed the following: