Taiwan PU Corporation TPU-B95 General Grade, Blow Molding Polyester Base TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Taiwan PU Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Taiwan PU Corporation TPU-B95 General Grade, Blow Molding Polyester Base TPU.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Blow MoldingInformation provided by Taiwan PU Corporation.
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
Tensile Strength at Break 37.27 MPa
5406 psi
Elongation at Break 600 %
600 %
100% Modulus 0.00780 GPa
1.13 ksi
300% Modulus 0.0118 GPa
1.71 ksi
Resilience 34
34
%, Impact Resilience
Taber Abrasion, mg/1000 Cycles 5.0
5.0
Processing Properties Metric English Comments
Feed Temperature 185 °C
365 °F
Middle Barrel Temperature 190 °C
374 °F
Compress zone
Front Barrel Temperature 195 °C
383 °F
Metering zone
Adapter Temperature 200 °C
392 °F
Die Temperature 200 °C
392 °F